15-7Mo 654SMO Ss Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
15-7Mo 654SMO Ss Pipe Application
15-7Mo 654SMO ss Pipe video
GNEE STEEL COMPANY
Our company is engaged in the production and trade of various 15-7Mo 654SMO Ss Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.
Refining, chemical equipment
Thermal power generation flue gas desulfurization equipment, wastewater treatment
Nuclear power generation, comprehensive utilization of coal, power generation energy field
Structures in the marine environment, seawater heat exchange industry
Paper industry, various bleaching equipment
Offshore platforms, stainless steel belt applications, subsea equipment
Chemical processing industry, pipeline industry
High-strength, corrosion-resistant mechanical equipment and components
15-7Mo 654SMO Ss Pipe Specification
| Element | Content (%) |
|---|---|
| Iron, Fe | Balance |
| Chromium, Cr | 14 -16 |
| Nickel, Ni | 6.50 - 7.75 |
| Molybdenum, Mb | 2 - 3 |
| Silicon, Si | 1 |
| Manganese, Mn | 1 |
| Aluminum, Al | 0.75 - 1.50 |
| Carbon, C | 0.09 |
| Phosphorus, P | 0.040 |
| Sulfur, S | 0.040 |
15-7Mo 654SMO ss Pipe


PH 15-7 Mo is a precipitation-hardened stainless steel used in applications requiring high strength and moderate corrosion resistance. Similar to 17-7, 2% molybdenum is used in place of 2% chromium, giving 15-7 Mo greater room and temperature strength. PH 15-7 Mo stainless steel can be formed in soft austenitic conditions and then hardened to high strength levels by low temperature heat treatment. This allows minimal distortion compared to other quenching and temper hardening processes. For maximum strength requirements, 15-7 Mo strip is available, heat treated with hard rolling condition C, condition CH900.
654SMo (S32654, 1.4652) super austenitic stainless steel is a super austenitic stainless steel containing 23% nickel, 25% chromium and 7% molybdenum. Its anti-corrosion ability is much better than ordinary austenitic steel. The smelting method of 654SMO super austenitic stainless steel: the currently popular argon-oxygen decarburization refining method abroad (VOD or AOD), and the continuous casting method of stainless steel can also be used.
Gnee Group participated in the NECC exhibition
Gnee Group participated in the NECC exhibition

Gnee Company Team
Gnee Company Team

Customer Case
customer visit


FAQ
Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.
Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: About the product price of 15-7Mo 654SMO ss Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.