GH3030 Plate
video

GH3030 Plate

Leading supplier of GH3030 (Alloy 75) high-temperature sheet metal. Excellent oxidation resistance, temperature resistance up to 1000℃, and superior weldability. We offer custom laser cutting and worldwide fast shipping. Inquire now for factory direct sales!
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH3030 Plate description

 

Inconel 600 Plate

GNEE GH3030 Alloy Plate

 

GH3030 sheet is a titanium-stabilized nickel-chromium-based solid solution strengthened superalloy. Globally recognized as an equivalent to Nimonic 75 (Alloy 75), it is the material of choice for engineers designing components that must withstand extreme temperatures and offer excellent machinability.

 

GH3030 alloy sheet possesses a stable microstructure and excellent oxidation resistance. It maintains its integrity at operating temperatures up to 800°C (1472°F) and resists oxidation at temperatures up to 1000°C (1832°F).

 

Gnee Steel, an ISO-certified professional supplier of GH3030 sheet, offers high-quality sheet that perfectly balances ductility, thermal fatigue resistance, and weldability.

 

Reduce material waste! We offer precision laser cutting, waterjet cutting, and plasma cutting services for GH3030 sheet metal based on your CAD drawings.

Get a custom quote for GH3030 sheet metal now

GH3030 Sheet Sizes and Availability

We offer a variety of GH3030 sizes to meet the needs of precision instrumentation and heavy industrial applications:

Cold-rolled sheet: Thickness 0.5 mm – 4.0 mm | Width up to 1000 mm.

Hot-rolled sheet: Thickness 4.0 mm – 50.0 mm | Width and length can be customized.

Surface treatments: Bright annealing (BA), pickling (No. 1), or sandblasting.

GH3030 Bright Annealed Steel Sheet (BA)
GH3030 Bright Annealed Steel Sheet (BA)
GH3030 Alloy Pickled (No.1) Plate
GH3030 Alloy pickled (No.1) plate
GH3030 sandblasting plate
GH3030 sandblasting plate

 

Specifications of GH3030 PLATES / SHEETS

 

Specifications of GH3030 PLATES
Grade GH3030
Thickness 0.1mm To 100 mm
Size 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Sheets, Plates, Coils, Slatting Coils, Perforated Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

High temperature alloy GH3030 Plate Specification

 

Chemical composition (%) of GH3030 alloy plate

Our GH3030 materials strictly adhere to GB/T 14992 and international equivalents.

Element Ni Cr Ti Al Fe C Mn Si P S
Percentage Bal 19.0-22.0 0.15-0.35 ≤ 0.15 ≤ 1.50 ≤ 0.12 ≤ 0.70 ≤ 0.80 ≤ 0.015 ≤ 0.010

 

Mechanical properties of GH3030 alloy plate (at room temperature)

Property Sheet Plate
Tensile Strength (Rm) ≥ 685 MPa ≥ 590 MPa
Yield Strength (Rp0.2) ≥ 295 MPa ≥ 245 MPa
Elongation (A5) ≥ 35% ≥ 35%
Hardness ≤ 200 HBW (Annealed) ≤ 200 HBW (Annealed)

 

Physical constants of GH3030 alloy plate

Physical Property Value
Density 8.4 g/cm³
Thermal Expansion (20-800°C) 16.5 × 10⁻⁶/K
Thermal Conductivity (100°C) 12.1 W/(m·K)

 

GH3030 Sheet & Plate Dimension Range

 

GH3030 Sheet & Plate Dimension Range

We provide GH3030 in both cold-rolled and hot-rolled conditions to support diverse industrial fabrication needs.

Product Form Thickness (mm) Width (mm) Length (mm) Typical Edge
Cold Rolled Sheet (CR) 0.5 mm – 4.0 mm 600 – 1000 2000 – 3000 Slit Edge / Mill Edge
Hot Rolled Plate (HR) 4.0 mm – 20.0 mm 1000 – 1500 2000 – 6000 Mill Edge / Cut Edge
Heavy Forged Plate 20.0 mm – 100.0 mm Custom Custom Machined / Sawn

We offer zero-loss solutions. We can use precision fiber laser or waterjet technology to cut GH3030 sheets to your exact CAD dimensions.

Request a Custom Cutting Quote

 

GH3030 Thickness Tolerance Tables (Technical Standard)

 

Dimensional consistency ensures reliable performance in high-velocity gas flow and pressure-bearing components.

Suitable for bright annealing (BA) and pickling surface treatments.

Specified Thickness (mm) Standard Tolerance (mm) High-Precision Grade (mm)
0.5 – 1.0 mm ± 0.08 ± 0.05
1.1 – 2.0 mm ± 0.12 ± 0.08
2.1 – 3.0 mm ± 0.15 ± 0.10
3.1 – 4.0 mm ± 0.18 ± 0.12

 

Suitable for annealing, pickling (No. 1) and sandblasting surface treatment.

Specified Thickness (mm) Tolerance (mm) Flatness Deviation (mm/m)
4.0 – 8.0 mm ± 0.35 ≤ 5.0
8.1 – 15.0 mm ± 0.45 ≤ 4.0
15.1 – 30.0 mm ± 0.60 ≤ 3.5
30.1 – 50.0 mm ± 1.20 ≤ 3.0

 

GH3030 alloy plate weight calculation reference

 

To assist in your logistics and engineering planning, use the following formula for GH3030 plates:

Density: 8.4 g/cm³

Formula: Weight (kg) = Thickness (mm) × Width (m) × Length (m) × 8.4

 

Planning a large-scale project? We offer tiered wholesale pricing for GH3030 steel plate orders over 500 kg.

View current bulk pricing for GH3030 plates

 

Gnee Steel: Full Range of GH3030 Products Available

 

You might need sheet metal today, but a complete project typically requires a unified source of materials. We offer a "one-stop" service for our full range of GH3030 products:

GH3030 Seamless Pipe
GH3030 seamless pipe
GH3030 Flange
GH3030 Flange
GH3030 Round Bar
GH3030 round bar
GH3030 Fasteners
GH3030 fasteners

 

GH3030 Sheet Shipping Time As Per Location

 

Price Changes
Extra 5 %
Export to Delivery Time in Days
Germany 21
Mexico 45
Canada 45
The Republic Of Congo 45-60
Gabon 45-60
Kazakhstan 20
Costa Rica 45
Panama 45
Puerto Rica 45
Jamaica 50
Equatorial Guinea 45-60
Norway 45
Bahamas 60
Trinidad And Tobago 60
Denmark 35

 

Products and services offered by Gnee Steel

 

GH3030 Plate Main Application Areas

 

Aerospace: Jet engine combustor linings, flame tubes, afterburner shells, and mounting rings.

Industrial Furnaces: Furnace chambers, radiant tubes, rotary kiln linings, and conveyor belts.

Heat Treatment: High-temperature fixtures, baskets, and gaskets.

Chemical Processing: High-temperature gas flow reactor linings and catalyst supports.

Applications of Inconel 600 Sheets

 
Combustion chamber lining
Combustion chamber lining
Industrial furnace furnace
Industrial furnace furnace
Heat treatment basket
Heat treatment basket
Reactor Lining
Reactor lining

 

Packaging method for Alloy 718 Pipe Fitting

Packaging method for Alloy 600 Plate

 

Gnee Steel uses the safest and most effective packaging methods for all types of cargo transportation. Our packaging methods include:

Wooden crates
Wooden pallets
Shrink wrap packaging
Cardboard boxes
Wooden crates (slatted)

 

About Gnee Steel

 

GH3030 Steel Sheet

 

Gnee Steel's GH3030 Steel Sheet

Ultra-Clean Melting: We use Vacuum Induction Melting (VIM) + Electroslag Remelting (ESR) processes to remove impurities, ensuring excellent thermal fatigue life.

Excellent Cold Formability: Our steel sheets undergo special annealing treatment, resulting in high plasticity, making them ideal for complex stamping, deep drawing, and spinning processes.

Weldability: GH3030 is arguably the easiest high-temperature alloy to weld (TIG welding, MIG welding, spot welding, seam welding), with weld efficiency almost equivalent to the base material.

Full Traceability: Each steel sheet comes with a Material Inspection Certificate (MTC) conforming to EN 10204 3.1, directly linked to the heat number.

VIM +  ESR Processes
VIM +  ESR processes
TIG welding
TIG welding
MIG welding
MIG welding

Gnee Steel GH3030 certificate

Gnee Steel GH3030 certificate

modular-1
Please contact us to get a quick quote for the GH3030 Plate you need

We supply these Alloy GH3030 Sheet and tubes according to DIN, ISO, JIS, or ANSI/ASME standards.

"We provide DDP/CIF shipping services to Germany and Italy."

FAQ

 

Q1: Can GH3030 plates be used in sulfur-containing environments?
A: Like most high-nickel alloys, GH3030 is sensitive to sulfidation in reducing atmospheres. It is best suited for oxidizing or neutral atmospheres. For sulfur-rich environments, please consult our engineers for specific coating or alloy alternatives.

 

Q2: What is the recommended heat treatment for GH3030 after cold forming?
A: We recommend a Solution Treatment at 1100°C - 1150°C followed by rapid air cooling or water quenching to restore ductility and optimal oxidation resistance.

 

Q3: How do your GH3030 plates compare to 310S Stainless Steel?
A: GH3030 is a nickel-based superalloy, whereas 310S is a high-alloy stainless steel. GH3030 has significantly better creep strength and does not suffer from the "sigma phase" embrittlement that can make 310S brittle after long-term service at 800°C.

 

Q4: Do you offer PVC coating for cold-rolled sheets?
A: Yes, we can apply single or double-sided PVC protective film to ensure your sheets arrive without a single scratch on the bright finish.

Hot Tags: gh3030 plate, China gh3030 plate suppliers, alloy cost, GH3030 High temperature alloy, toughness alloy, alloy fair, alloy feature, surface treatment alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry