2.4669 Nickel Base Superalloy Plate
video

2.4669 Nickel Base Superalloy Plate

Nickel (plus cobalt)…70.00 minutes
Chromium…14.0-17.0
Iron…5.0-9.0
Titanium…2.25-2.75
Aluminum…0.40-1.00
Niobium (plus tantalum)…0.70-1.20
Manganese…1.00 Max.
Silicon…below 0.50
Sulfur…below 0.01
Copper…0.50 or less
Carbon…0.08 or less
Cobalt 1 …1.00 Max
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
2.4669 Nickel Base Superalloy Plate

 2.4669 Nickel Base Superalloy Plate Video

2.4669 Nickel Base Superalloy Plate is a corrosion-resistant, oxidation-resistant, high-strength precipitation hardening alloy. It is mainly a nickel-based high-temperature alloy that is age-strengthened with the γ" phase. The service temperature is below 800°C. The alloy has good corrosion resistance and oxidation resistance below 980°C, and has high strength below 800°C. It has good creep resistance below 700℃ and good relaxation resistance below 540℃. It also has good formability and welding performance. The alloy is in solid solution state and is pure austenite. body tissue.

 

2.4669 Nickel Base Superalloy Plate

 

Grade

Ni%

Cr%

Nb%

Fe%

Al%

Ti%

C%

Mn%

Si%

Cu%

S%

Co%

Inconel X750

Max 70

14-17

0.7-1.2

5.0-9.0

0.4-1.0

2.25-2.75

Max 0.08

Max 1.00

Max 0.50

Max 0.5

Max 0.01

Max 1.0

 

2.4669 Nickel Base Superalloy Plate Application

 

  • Rocket construction
  • Components for gas turbines
  • Nuclear reactors
  • Tools
  • Aircraft structure

 

Gnee Company Team

Gnee Company Team

24669 Nickel Base Superalloy Plate team

38000㎡ workshop and 200+ emplovees to meet your huge demands.

 

2.4669 Nickel Base Superalloy Plate Packing & Delivery

2.4669 Nickel Base Superalloy Plate Packing & Delivery

24669 Nickel Base Superalloy Plate packing

 

Export standard packaging, bundling or as required.

The internal dimensions of the container are as follows:

20ft GP: 5.9m (length) x 2.13m (width) x 2.18m (height) approximately 24-26CBM

40ft GP: 11.8m (length) x 2.13m (width) x 2.18m (height) approx. 54CBM

40ft HG: 11.8m (length) x 2.13m (width) x 2.72m (height) approx. 68CBM

 

Customer Visit

Customer Visit

24669 Nickel Base Superalloy Plate customer visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ

 

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.

 

Q: How long is your delivery time?

A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.

 

Q: Do you provide samples ? is it free or extra ?

A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

 

Q: What is your terms of payment ?

A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable

 

Hot Tags: 2.4669 nickel base superalloy plate, China 2.4669 nickel base superalloy plate suppliers, alloy event, competitive alloy, alloy organization, homogeneity alloy, alloy review, alloy improvement

Send Inquiry

whatsapp

Phone

E-mail

Inquiry