GH4169 Nickel Alloy Belt For Petrochemical Industrial Reactors
video

GH4169 Nickel Alloy Belt For Petrochemical Industrial Reactors

Specifications: GH4169, GH169, Inconel718, N07718, W.Nr.2.4668, NiCr19Fe19Nb5Mo3, NA 51, NC19FeNb
Standard: GB/T14992-2005
Certification: ISO9001:2015
Features: Excellent creep rupture strength, reaching over 140 MPa at 700℃, ensuring excellent long-term stability in high-temperature environments.
Applications: Aerospace, chemical, shipbuilding, and other industries.
Product Forms: Wire, strip, bar, tube, plate
Minimum Order Quantity: 200KG
Payment Methods: Wire Transfer (T/T), Letter of Credit (LC)
Price: Negotiable
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH4169 high temperature alloy aerospace coil description

GH4169 high temperature alloy aerospace coil

GNEE GH4169 high temperature alloy aerospace coil

 

GH4169 nickel alloy strip is highly suitable for petrochemical reactors due to its excellent high-temperature strength, creep resistance, and corrosion resistance, making it particularly suitable for harsh chemical environments. Its key properties include high tensile and fatigue strength up to 700℃, good oxidation and corrosion resistance up to 1000℃, and stable chemical properties, enabling reliable operation under the high-stress, high-temperature conditions commonly encountered in petrochemical processing. This alloy is also renowned for its excellent weldability and comprehensive performance over a wide temperature range of -253℃ to 650℃.

 

Specification Of GH4169 nickel alloy belt for petrochemical industrial reactors

 

Product Name GH4169 Nickel Alloy Strip
Grades Inconel alloy 718 / UNS N07718 / W.Nr. 2.4668
Hardness 70-90HRB
Thickness 0.10mm-3.0mm
Width 1.0mm-600mm
Edge Slit/Deburred/Round
Quantity Tolerance ±10%
Paper Core Internal Diameter Ø 200mm, Ø300mm, Ø400mm, Ø500mm paper core, special internal diameter core and without paper core on customer request
Surface Finish The alloy strip foil has a smooth surface, free from scratches and impurities
Applications See Below Information
Packaging Wooden Pallet/Wooden Case
Payment Terms 30% TT deposit and 70% balance before shipment, 100% LC at sight
Delivery Time 15-20 working days
MOQ 500 kgs

 

GH4169 nickel alloy belt for petrochemical industrial reactors Specification

 

GH4169 Nickel Alloy Strip Chemical Compositions

Grade Standard C Si Mn P S Cr Ni Ti
GH4169/INCONEL 718 ASTM B 670 ≤0.08 ≤0.35 ≤0.35 ≤0.015 ≤0.015 17.00-21.00 50.0-55.0 0.65-1.15

 

GH4169 Nickel Alloy Strip Mechanical Properties

Element Yield Strength (0.2%Offset) Melting Point Density Tensile Strength Elongation
GH4169/718 MPa – 1034 1336 °C (2437 °F) 8.19 g/cm3 MPa – 1241 Min 10 %

 

GH4169 Nickel Alloy Strip Equivalent Grades

CHINA STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN OR
GH4169 2.4668 N07718 – – – – – –

 

application Of GH4169 nickel alloy belt for petrochemical industrial reactors

 

GH3652 High-Temperature Alloy Steel Pipes For Chemical Processing Plants

Applications in Petrochemical Reactors

Structural Components: High-stress, high-temperature components inside reactor vessels.

Pipelines and Equipment: Their excellent corrosion resistance makes them ideal for pipelines, heat exchangers, and other equipment handling corrosive chemicals.

Downstream Processing: Suitable for other parts of the plant, such as gas turbines and oil and gas field equipment, where operating conditions are extremely harsh.

 

GH4169 nickel alloy belt for petrochemical industrial reactors production process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel provides the following heat treatments for GH4169 nickel alloy belt for petrochemical industrial reactors: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

Key Features of GH4169 nickel alloy belt for petrochemical industrial reactors

 

High Temperature Performance: Maintains high tensile strength, fatigue strength, and creep strength at temperatures up to 700°C, and excellent oxidation resistance at temperatures up to 1000°C.

Corrosion Resistance and Oxidation Resistance: Exhibits excellent resistance to stress corrosion cracking and pitting corrosion, as well as superior high-temperature oxidation resistance.

Mechanical Strength: Utilizes a precipitation-strengthened nickel-based superalloy structure, resulting in high yield strength and tensile strength.

Wide Temperature Range: Maintains good strength and ductility from low temperatures up to 650°C.

Weldability: Exhibits excellent weldability, crucial for manufacturing complex components such as reactors.

Reliability: Offers excellent durability and reliability in harsh environments, reducing the need for frequent replacements.

 

GH4169 nickel alloy belt for petrochemical industrial reactors Packaging 

 

gh4169 nickel alloy strip packaging

Standard Export Sea Freight Packaging:

Waterproof paper roll + PVC film + strapping + wooden pallet or crate;

Customized packaging available upon request (logo or other content can be printed on the packaging);

Other special packaging designs available upon request;

Wall-mounted and skylight transport available;

International Express: DHL/UPS/FEDEX/EMS and our own dedicated line;

Air or Sea Freight;

Port of Loading: Shanghai, Ningbo, or as per your requirements.

 

About Gnee Steel

00

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

FAQ

Q:What is the maximum temperature resistance of GH4169 high-temperature alloy steel coils and strips?

A: GH4169 can withstand temperatures up to 900°C (1,652°F), making it ideal for high-temperature applications such as aerospace and power generation components.

Q:What are the main characteristics of GH4169 high-temperature alloy steel?

A: GH4169 possesses excellent high-temperature resistance, superior tensile strength, outstanding oxidation resistance, and durability under extreme conditions, ensuring reliable operation in demanding applications.

Q:In which industries can GH4169 be used?

A: GH4169 is widely used in industries such as aerospace, power generation, petrochemicals, and shipbuilding, where extremely high strength, heat resistance, and corrosion resistance are required.