GH2901 Alloy Bar
video

GH2901 Alloy Bar

GH2901 is an austenitic age-hardening alloy. Has a high yield strength and lasting strength. Good oxidation resistance, long-term use of tissue stability. Widely used in aviation and ground gas turbine engine rotating disk (turbine plate, compressor plate, shaft diameter, etc.), static structure, turbine outer ring and fasteners and other parts.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH2901 (GH901) nickel-based alloy rod has good high temperature strength and can maintain high yield strength and tensile strength at temperatures up to 1093°C (2000°F). This makes it very suitable for structures and components at high temperatures. GH2901 alloy rod has excellent creep resistance and can withstand continuous stress for a long time at high temperatures without deformation or failure. This makes it more reliable for applications in high temperature environments, such as gas turbines, aircraft engines, etc.

GH2901 Application:Iron-based superalloy

Category Type Grade Designations
Grades Superalloys GH2901 China - GB ,

Chemical composition(wt.%) of GH2901 grade:

Elements Min.(≥) Max.(≤)
C 0.02 0.06
Cr 11.0 14.0
Mo 5.0 6.5
Ni 40.0 45.0
Al - 0.3
Ti 2.8 3.1
B 0.001 0.02
Mn - 0.4
Fe - Remainder

Mechanical properties of grade GH2901

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
677 (≥) 666 (≥) 21 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade GH2901

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
291 (≥) 572 (≥) 33 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
         
626 659 514  

 nickel super alloy

GH2901 alloy Bar has the following physical properties:

Density: The density of GH2901 alloy is about 8.19 g/cm3, which is relatively high.

Melting point: The melting point of GH2901 alloy is about 1260-1340 degrees Celsius, which has a high melting point.

Thermal conductivity: The thermal conductivity of GH2901 alloy is about 9.8 watts/meter·Kelvin at room temperature, which has good thermal conductivity.

Coefficient of thermal expansion: The linear thermal expansion coefficient of GH2901 alloy is about 12.8 x 10^-6/degree Celsius, which is similar to many metals.

Elastic modulus: The elastic modulus of GH2901 alloy is about 204 gigapascals, indicating that it has good elastic properties.

Resistivity: The resistivity of GH2901 alloy is about 1.3 x 10^-6 ohm·meter, which has a low resistivity.

Packaging&shipping

ni superalloy GH2901

Hot Tags: gh2901 alloy bar, China gh2901 alloy bar suppliers, alloy advertising, fracture toughness alloy, base alloy, alloy competitor, 2 4669 sheet stainless steel, alloy feedback

Send Inquiry

whatsapp

Phone

E-mail

Inquiry