2J31 3J40 Alloy Pipe
video

2J31 3J40 Alloy Pipe

2J31 permanent magnet alloy is mainly composed of iron, cobalt, nickel and copper. Its processing technology includes steps such as powder metallurgy and hot pressing, and the required magnetic properties are obtained through high-temperature heat treatment and cooling.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
2J31 3J40 Alloy Pipe Application

2J31 3J40 Alloy Pipe video

GNEE STEEL COMPANY

Our company is engaged in the production and trade of various 2J31 3J40 Alloy Pipe, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.

Due to its excellent magnetic and mechanical properties, 3J40 alloy is widely used in many fields, including:
Magnetic recording media: As an important component of magnetic recording media such as disks and tapes, 3J40 alloy can store and read large amounts of data. It has the characteristics of high density, high speed and low noise, which has led to the rapid development of magnetic storage technology.
-Sensor technology: Because 3J40 alloy has low coercivity and high sensitivity, it can be used to manufacture equipment such as magnetic sensors and magnetic switches. It has important application value in fields such as automation control, electronic vehicles and smart homes.
Power engineering: 3J40 alloy is widely used in power engineering such as generators, transformers and magnetic control equipment. Its high saturation magnetic induction intensity and good thermal stability can improve the efficiency and reliability of the equipment.

2J31 3J40 Alloy Pipe Specification

 

Brands Chemical analysis
C S P Mn Si Ni Cr Co V
≤
2J3l ≤O.12 0.020 O.025 ≤0.70 ≤O.70 ≤O.7 - 51.O~53.0 10.8~
11.7
2J32 ≤O.12 0.020 0.025 ≤O.70 ≤O.70 ≤0.7 - 51.O~53.O 11.8~12.7
2J33 ≤O.12 0.020 O.025 ≤O.70 ≤O.70 ≤0.7 - 51.O~
53.O
12.8~13.8

2J31 3J40 Alloy Pipe

2J31 3J40 Alloy Pipe2J31 3J40 Alloy Pipe

2J31 permanent magnet alloy is mainly composed of iron, cobalt, nickel and copper. Its processing technology includes steps such as powder metallurgy and hot pressing, and the required magnetic properties are obtained through high-temperature heat treatment and cooling. 2J31 permanent magnet alloy has high coercivity, high remanence and good corrosion resistance, and is suitable for applications in motors, sensors and other fields.
3J40 elastic alloy is a high-hardness, high-elastic alloy material developed by China in the process of imitating the former Soviet Union's brand 40XHIO (0Cr40Ni55AI3). The strength of this alloy is extremely high, reaching more than 1900 MPa, and the hardness is also quite high, reaching 780 Hv. This hardness and strength make 3J40 alloy an important material that is wear-resistant, corrosion-resistant and non-magnetic. In precision instrument manufacturing, 3J40 alloy is widely used to manufacture elastic components, such as elastic sensors, energy storage components, frequency components and other precision devices.

 

2J31 3J40 Alloy Pipe process & size

2J31 3J40 Alloy Pipe process & size

2J31 3J40 Alloy Pipe process & size

2J31 3J40 Alloy Pipe process & size

 

Customer Case

 

 

customer visit

2J31 3J40 Alloy Pipe

2J31 3J40 Alloy Pipe

FAQ

 

 

 

 

 

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: About the product price of 2J31 3J40 Alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.