Grade: GH3030
Surface Treatment: 2B, 2D, BA NO(8)
Shape: Round, Square, Rectangular
Type: Seamless

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

High-temperature alloy GH3030 seamless nickel alloy tube description

GH3030 alloy thin-walled thick-walled tube

GNEE High-temperature alloy GH3030 seamless nickel alloy tube

 

GH3030 seamless nickel-based alloy tube is a type of nickel-based alloy tube characterized by high thermal strength, excellent oxidation resistance, and good thermal fatigue performance below 800℃. It is renowned for its stable austenitic structure, good plasticity, and excellent cold stamping and welding properties. Its high-temperature strength and corrosion resistance make it suitable for applications in aerospace, gas turbines, chemical engineering, and nuclear energy, where it can withstand high-temperature and corrosive environments.

GH3030 thin-walled tube is a high-performance metal tube designed to withstand harsh environments such as high temperature, high pressure, and strong corrosion. Utilizing advanced manufacturing processes, it ensures the integrity and uniformity of the tube, eliminates weld joints, and offers higher strength and reliability.

 

GH3030 thin-walled tube employs a nickel core structure, with nickel boasting a melting point of nearly 1300 degrees Celsius. It exhibits excellent thermal strength, performing admirably within a plastic deformation range of 800 degrees Celsius, with a bending strength reaching 90 degrees Celsius. It also possesses superior oxidation and corrosion resistance, withstanding media temperatures up to 900 degrees Celsius. Furthermore, GH3030 thin-walled tube is resistant to oxidizing gases, sulfides, chlorides, and other corrosive substances. This characteristic gives it a significant advantage in the chemical and petrochemical industries.

 

The characteristics of GH3030 thin-walled tube include small tolerances, high precision, a smooth surface, and the absence of sharp peeling and rolling marks. The coil material is designed to prevent "chain knife bending" and is stretched to near-ideal straight-line angles with minimal deviation. Its bent sections exhibit good cold-welding properties and are also suitable for other processing techniques such as drawing and rolling. Furthermore, GH3030 thin-walled tubes are suitable for argon arc welding, spot welding, seam welding, and brazing, making them a material with excellent weldability.

Specification Of High-temperature alloy GH3030 seamless nickel alloy tube

 

Specifications Of GH3030 Thin Wall Thickness Tube

Type:

Seamless

Surface Treatment:

Polished

Inner diameter:

Customized

Outer diameter:

Customized

Wall thickness:

Customized

Length:

Customized

Origin:

China

Material:

Alloy

Standard:

ASTM, AISI

Sample:

Avaliable

 

High-temperature alloy GH3030 seamless nickel alloy tube Specification

 

GB/T 15062 GH3030 / Ni80Cr20 Nickel Alloy Tube Equivalent Material

Standard GB/T 15062
Material GH3030 (GH 30)
Equivalent Material ЗИ435,XH78T


GB/T 15062 GH3030 / Ni80Cr20 Nickel Alloy Tube Chemistry Composition

C

Cr

Ni

Ti

Al

Fe

Mn

Si

P

S

≤0.12

19.0~22.0

Balance

0.15~0.35

≤0.15

≤1.5

≤0.7

≤0.8

≤0.03

≤0.02


GB/T 15062 GH3030 / Ni80Cr20 Nickel Alloy Tube Mechanical Properties

Yield Rp0.2, Mpa

Tensile Rm, MPa

Impact KV/Ku, J

Elongation,
A%

Reduction in cross section on fracture,Z%

As-Heat-Treated Condition

Brinell hardness, HBW

963 (≥)

953 (≥)

33

23

33

Solution and Aging, Annealing, Ausaging, Q
+T, etc

424








GB/T 15062 GH3030 / Ni80Cr20 Nickel Alloy Tube Physical Properties

Temperature
(℃)

Modulus of elasticity
(GPa)

Mean coefficient of thermal
expansion 10-6/(℃) between 20(℃) and

Thermal conductivity
(W/m·℃)

Specific thermal capacity (J/kg·℃)

Specific electrical resistivity (Ωmm²/m)

Density
(kg/dm³)

Poisson's
coefficient

21 - -     0.23 -  
984 459 - 13.3 311   -  
996 - 34 44.2     223 123

 

Features Of GH3030 Thin Wall Thickness Tube

 

product-604-691

1. Excellent Strength Characteristics at High Temperatures: GH3030 thin-walled tubes exhibit good thermal strength and ductility below 800 degrees Celsius. Furthermore, they maintain their mechanical properties even at high temperatures.

2. Excellent Corrosion Resistance: GH3030 thin-walled tubes demonstrate excellent corrosion resistance even in highly corrosive environments such as oxidizing atmospheres, sulfide environments, and chloride environments. Therefore, GH3030 thin-walled tubes are widely used in chemical and petrochemical industries due to their superior performance. Their long-term stability also makes them suitable for long-term operation.

3. Excellent Surface Finish: GH3030 thin-walled tubes have extremely high dimensional accuracy and a smooth, delicate surface free from defects such as peeling and rolling marks. Slight deviations in the coil during straightening indicate that vertical rolling is an ideal choice.

 

High-temperature alloy GH3030 seamless nickel alloy tube Surface Treatments

  • Pickling treatment
    Gnee Steel
    Pickling treatment
  • Mirror polishing treatment
    Gnee Steel
    Mirror polishing treatment
  • Polishing treatment
    Gnee Steel
    Polishing treatment
  • Sandblasting treatment
    Gnee Steel
    Sandblasting treatment

Gnee Steel provides four surface treatments for High-temperature alloy GH3030 seamless nickel alloy tube: pickling, mirror polishing, polishing, and sandblasting.

 

High-temperature alloy GH3030 seamless nickel alloy tube production process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel provides the following heat treatments for High-temperature alloy GH3030 seamless nickel alloy tube: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

High-temperature alloy GH3030 seamless nickel alloy tube Packaging 

  • Steel strapping
    Gnee Steel
    Steel strapping
  • Wooden boxes/crates
    Gnee Steel
    Wooden boxes/crates
  • Rainproof cloth packaging
    Gnee Steel
    Rainproof cloth packaging
  • Airworthy export packaging 

     

     

    Gnee Steel
    Airworthy export packaging 

In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.

 

 

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Hot Tags: gh3030 alloy thin-walled thick-walled tube, China gh3030 alloy thin-walled thick-walled tube suppliers, alloy strip, industrial alloy, alloy fair, alloy part, oil and gas alloy, alloy success story

Send Inquiry

whatsapp

Phone

E-mail

Inquiry