GH2132 High Temperature Alloy Seamless Tube
video

GH2132 High Temperature Alloy Seamless Tube

GH2132 tubing is widely used in various high-temperature environments, such as gas turbines and other aerospace components.
Grade: GH2132
Length: Customizable
Shape: Round, Square, Rectangular
Type: Seamless
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH2132 high temperature alloy seamless tube description

GH2132 high temperature alloy seamless tube

GNEE GH2132 high temperature alloy seamless tube

 

GH2132 is a high-temperature alloy, also known as UNS 66286 or A-286, used to manufacture seamless steel tubes for high-stress applications. It is an iron-nickel-chromium-based high-temperature alloy with added elements such as molybdenum, titanium, and aluminum for strengthening. This seamless steel tube is favored for its excellent high-temperature strength and creep resistance below 650°C (1200°F), as well as good corrosion resistance and weldability.

GH2132 Production Standard

Alloy Seamless Pipe and Tube Welded Pipe and Tube Plate, Sheet, and Strip Forging
GH2132 GJB 3317, GB/T 14995, GB/T 14996 GB/T 15062 GJB 2611, GJB 2612, GJB 3167, Q/3B4701, Q/6S1032 GJB 3065, GJB 3782

 

Specification Of GH2132 high temperature alloy seamless tube

 

Specifications of High Temperature Gh2132 PIPES / TUBE:
Grade High Temperature Gh2132
Range 1/2″ Nominal Bore To 16″Nominal Bore
Length Single Random, Double Random & Cut Length.
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Round, Square, Rectangular, Hydraulic Etc
Type Seamless / ERW / Welded / Fabricated / EFW
Applications Off-Shore Oil Drilling Companies, Power Generation, Petrochemicals, Gas Processing, Specialty Chemicals, Pharmaceuticals, Pharmaceutical Equipment, Chemical Equipment, Sea Water Equipment, Heat Exchangers, Condensers, Pulp and Paper Industry

 

GH2132 high temperature alloy seamless tube Specification

 

Chemical composition of High Temperature Alloy GH2132(%)

Element Percentage (%)
Nickel (Ni) 24.0 – 27.0
Chromium (Cr) 13.5 – 16.0
Iron (Fe) Balance
Molybdenum (Mo) 1.0 – 1.5
Titanium (Ti) 1.9 – 2.35
Vanadium (V) 0.1 – 0.5
Aluminum (Al) 0.35 max
Carbon (C) 0.08 max
Manganese (Mn) 2.0 max
Silicon (Si) 1.0 max
Phosphorus (P) 0.025 max
Sulfur (S) 0.025 max
Boron (B) 0.001 – 0.010

 

Physical properties of High Temperature Alloy GH2132

Physical Property Value Unit
Density 7.93 g/cm³
Melting Point 1364 – 1424 °C
Specific Heat Capacity 0.461 J/g·K
Thermal Conductivity 14.9 W/m·K
Coefficient of Expansion 16.4 (at 20-100°C) µm/m·K
Electrical Resistivity 1.29 µΩ·m

 

Mechanical properties of High Temperature Alloy GH2132

Mechanical Property Value at Room Temperature Value at Elevated Temperature (e.g., 650°C) Unit
Tensile Strength 850 – 1100 550 – 800 MPa
Yield Strength (0.2% Offset) 550 – 750 230 – 550 MPa
Elongation 25 – 40 20 – 30 %
Hardness 24 – 38 – Rockwell C

 

Application of high temperature alloy GH2132 seamless steel pipe

 

Aerospace Industry: GH2132 high-temperature alloy is widely used in the aerospace industry for manufacturing jet engine components, turbine blades, and afterburner components. Its ability to maintain strength at high temperatures and its excellent oxidation resistance make it ideal for these applications.

Gas Turbines: GH2132 is used to manufacture internal components of gas turbines, such as blades, rings, and casings, thanks to its excellent high-temperature strength and corrosion resistance, ensuring service life and reliability under extreme conditions.

Automotive Industry: In high-performance automotive applications, GH2132 is used to manufacture exhaust components and turbocharger components, which are exposed to high-temperature environments and require materials that can maintain their performance under thermal stress.

Fasteners: GH2132 is commonly used to produce high-temperature fasteners, including bolts, nuts, and screws, which are widely used in various industrial sectors requiring high strength and heat resistance.

Nuclear Applications: The alloy's excellent stability at high temperatures and its resistance to radiation and corrosion make it suitable for nuclear reactors, and especially for non-reactor components subjected to high temperatures. Petrochemical Industry: In petrochemical plants, the high-temperature alloy GH2132 is used in pipelines, valves, and reactor components, applications requiring materials capable of withstanding corrosive substances and high-temperature environments.

Industrial Furnaces: Components within industrial furnaces, such as furnace baskets and trays, can be manufactured using GH2132 to fully utilize its high-temperature strength and oxidation resistance, ensuring durability and performance under harsh thermal conditions.

The unique combination of high-temperature strength, oxidation resistance, and corrosion resistance makes GH2132 an ideal material for components subjected to extreme thermal and corrosive conditions.

 

GH2132 high temperature alloy seamless tube Surface Treatments

  • Pickling treatment
    Gnee Steel
    Pickling treatment
  • Mirror polishing treatment
    Gnee Steel
    Mirror polishing treatment
  • Polishing treatment
    Gnee Steel
    Polishing treatment
  • Sandblasting treatment
    Gnee Steel
    Sandblasting treatment

Gnee Steel provides four surface treatments for GH2132 high temperature alloy seamless tube: pickling, mirror polishing, polishing, and sandblasting.

 

GH2132 high temperature alloy seamless tube production process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel provides the following heat treatments for GH2132 high temperature alloy seamless tube: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

GH2132 high temperature alloy seamless tube Packaging 

  • Steel strapping
    Gnee Steel
    Steel strapping
  • Wooden boxes/crates
    Gnee Steel
    Wooden boxes/crates
  • Rainproof cloth packaging
    Gnee Steel
    Rainproof cloth packaging
  • Airworthy export packaging 

     

     

    Gnee Steel
    Airworthy export packaging 

In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.

 

 

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Hot Tags: gh2132 high temperature alloy seamless tube, China gh2132 high temperature alloy seamless tube suppliers, alloy feature, nickel based superalloy, plasticity alloy, alloy optimization, high purity alloy, machining alloy

Send Inquiry

whatsapp

Phone

E-mail