2J52 6J22 Large Diameter Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
super alloy Products Application
2J52 6J22 Large diameter Pipe Video
6J22 alloy is widely used in the production of miniature high-resistance precision wire-wound resistors, precision resistors, sliding wire resistors, standard resistors, self-compensating resistance strain gauges below 400°C and other special resistance components in instruments and meters.
Application fields of 2J52: 2J52 is widely used in motors, power generation, sensors and other fields, and is especially suitable for occasions where stable magnetic properties and high temperature resistance are required.
super alloy Material Specification
|
Grade |
C |
Si |
Mn |
P |
S |
Ni |
Al |
Fe |
Cr |
|
6J22 |
≤0.04 |
≤0.20 |
0.5~1.05 |
≤0.010 |
≤0.010 |
Bal. |
2.7~3.2 |
2.0~3.0 |
19.0~21.5 |
2J52 6J22 Large diameter Pipe


2J52 is an alloy material with excellent magnetic and mechanical properties, mainly composed of iron, nickel, aluminum, molybdenum, copper and other elements. It has high coercivity, low hysteresis, good magnetic permeability and oxidation resistance, making it an ideal permanent magnet material.
6J22 Karma alloy is mainly composed of nickel, chromium, aluminum and iron. The resistivity is about three times higher than that of manganese-copper, and it has a lower temperature coefficient of resistance and a low thermoelectric potential against copper. It has good long-term resistance stability and anti-oxidation properties. The operating temperature is wider than that of manganese copper. Suitable for making precision micro-resistance components and strain gauges.
Customer Case
customer visit


FAQ
Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.
Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.
Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.
Q: About the product price of 2J52 6J22 Large diameter Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: 2j52 6j22 large diameter pipe, China 2j52 6j22 large diameter pipe suppliers, alloy attribute, alloy feedback, Gh3030 High Temperature Alloy Pipe, non magnetic alloy, high purity alloy, alloy ingot