GH1140 Alloy Bar
video

GH1140 Alloy Bar

GH1140 is a solid solution strengthened iron-nickel-based superalloy, in addition to a large number of chromium, and with a small amount of tungsten, molybdenum, aluminum and titanium and other elements to strengthen the solid solution.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH1140 alloy is a high-performance nickel-based alloy, mainly based on nickel and chromium, which is commonly used in applications requiring good high-temperature properties and machinability. It is very important in industrial applications, especially in those where high temperature resistance, corrosion resistance and good mechanical properties are required.The main components of the GH1140 alloy include nickel and chromium, and may also contain other elements such as iron, molybdenum and titanium, which together give the alloy excellent high temperature properties and good mechanical properties. The ratio of nickel to chromium and the addition of other alloying elements play a decisive role in the overall properties of the alloy.

GH1140 Chemical Composition

element

C

Cr

In

IN

Mo

Al

Of

Mass fraction/%

0.06-0.12

20.00-23.00

35.00-40.00

1.40-1.80

2.00-2.50

0.20-0.60

0.70-1.20

element

Fe

This

Mn

And

P

S

 

Mass fraction/%

Remain

≤0.050

≤0.70

≤0.80

≤0.025

≤0.015

 

GH1140 physical and mechanical properties

density

Melting point

8.09g/cm³

-

super alloy metals GH1140

GH1140 Bar features

GH1140 alloy rod has good process performance and can be hot processed and cold processed. In terms of hot processing, the alloy has good plasticity and can withstand various hot processing processes, such as casting, forging, welding, etc. In terms of cold processing, the alloy can be rolled, drawn, stamped and other processes to obtain products of various shapes and specifications.

application of superalloy gH1140 bar

Due to the excellent high temperature performance and corrosion resistance of GH1140 alloy rod, it is widely used in aviation, aerospace, energy and other fields. In the aviation field, the alloy can be used to manufacture high temperature parts of aerospace engines, such as combustion chambers, turbine blades, etc.; in the aerospace field, the alloy can be used to manufacture high temperature parts of rocket engines, such as nozzles, combustion chambers, etc.; in the energy field, the alloy can be used to manufacture parts in high temperature reactors, such as fuel rods, control rods, etc.

Packaging&Shipping

sss super alloys GH1140

Hot Tags: gh1140 alloy bar, China gh1140 alloy bar suppliers, alloy company, modulus of elasticity alloy, Heat Resistant Steel, alloy cost, stable alloy, 2 4669 stainless steel plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry