Alloy 825, 2.4858, UNS N08825, Incoloy 825 – Description
Alloy 825 (N08825) is a member of the Ni-Cr-Fe-Mo family of alloys developed in the 1950s. It contains nominally 42% Ni, 32% Fe, 22% Cr, 2.5% Mo and 2% Cu, stabilized with 0.8% Ti, which gives it excellent resistance to sulfuric acid and phosphoric acid. The alloy is resistant to many types of corrosion. Corrosive environment and intergranular sensitization. Resistant to oxidizing and reducing acids, SCC, pitting and intergranular corrosion for use in chemical and petrochemical processing, oil and gas extraction, pollution control, waste treatment and pickling applications

What is uns N08825 standard?

What is uns N08825 standard?

Application areas
Alloy 825 is used in phosphoric acid evaporators, pickling equipment, chemical processing vessels and pipelines, spent nuclear fuel recovery equipment, propeller shafts, and tank trucks

N08825-Physical and mechanical properties
Physical properties at room temperature: Density: 8.14 g/cm3 Linear expansion coefficient: 14.0 *10-6m/(m*K) Thermal conductivity: 11.1 W/(m*K) Specific heat capacity: 440 J/(kg*K) Young's modulus : 195 GPa Resistivity: 1127 μΩ*m Magnetic permeability: 1.005 Curie temperature: -196 °C Melting temperature: 1370-1400 °C Mechanical properties of annealed Incoloy 825 rod: Yield strength: 324 MPa Tensile strength Rm: 690 MPa Elongation: 45 % Hardness: 90 Impact energy KV of HRBI annealed alloy 825 plate as a function of temperature: Impact energy KV 20°C: 107-113 J Impact energy KV -79°C: 106 J Impact energy KV -196°C: 91-97 J Impact energy KV -253°C: 92 J Tensile strength and temperature: Ambient temperature: 693 MPa 93°C: 655 MPa 204°C: 637 MPa 316°C: 632 MPa 371° C: 621 MPa 427° C: 610 MPa 482°C: 608 MPa 538°C: 592 MPa 593°C: 541 MPa 649°C: 465 MPa 760°C: 274 MPa 871°C: 135 MPa 982°C: 75 MPa 1093°C: 42 MPa Yield strength and temperature: Ambient temperature: 301 MPa 93°C: 279 MPa 204°C: 245 MPa 316°C: 232 MPa 371°C: 234 MPa 427°C: 228 MPa 482°C: 221 MPa 538°C C: 229 MPa 593°C: 222 MPa 649°C: 213 MPa 760°C: 183 MPa 871°C: 117 MPa 982°C: 47 MPa 1093°C: 23 MPa Elongation and temperature: At ambient temperature: 43 % 538 °C: 43 % 593°C: 38 % 649°C: 62 % 760°C: 87 % 871°C: 102 % Thermal expansion coefficient and temperature (linear): 24-93°C: 14.0 μm/( m *K) 24-205°C: 14.9 μm/(m*K) 24-315°C: 15.3 μm/(m*K) 24-425°C: 15.7 μm/(m*K) 24-540° C : 15.8 μm/(m*K) 24-650°C: 16.4 μm/(m*K) 24-760°C: 17.1 μm/(m*K) 24-870°C: 17.5 μm/(m* K) ) Thermal conductivity and temperature: at ambient temperature: 11.1 W/(m*K) 93℃: 12.3 W/(m*K) 205℃: 14.1 W/(m*K) 315℃: 15.8 W/(m *K) 425°C: 17.3 W/(m*K) 540°C: 18.9 W/(m*K) 650°C: 20.2 W/(m*K) 760°C: 22.3 W/(m*K ) K) 870°C: 24.8 W/(m*K) 980°C: 27.7 W/(m*K) Resistivity and temperature: at ambient temperature: 1127 μΩ*m 93°C: 1142 μΩ*m 205° C: 1180 μΩ*m 315°C: 1210 μΩ*m 425°C: 1248 μΩ*m 540°C: 1265 μΩ*m 650°C: 1267 μΩ*m 760°C: 1272 μΩ*m 870°C: 1288 μΩ*m 980°C: 1300 μΩ*m