GH4080A Alloy Seamless Tubes For Power Plants
video

GH4080A Alloy Seamless Tubes For Power Plants

GH4080A Seamless Tube Performance
Corrosion Resistance: Excellent oxidation and corrosion resistance.
High Temperature Performance: This alloy is designed for operating temperatures up to 800°C (1472°F) and exhibits excellent creep resistance in the 650°C to 850°C range.
Machining Properties: Good hot and cold working properties. Equivalent Grade: Similar to Nimonic 80A alloy.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH4080A alloy seamless tubes for power plants description

GH4080A alloy seamless tubes for power plants

GNEE GH4080A alloy seamless tubes for power plants

 

GH4080A is a nickel-chromium-cobalt alloy widely used in seamless steel pipes for power plants due to its high strength and creep resistance at high temperatures, as well as excellent corrosion resistance, oxidation resistance, and sulfidation resistance. These pipes are manufactured without weld seams, thus improving strength and reliability for high-pressure applications, and must meet specific standards, such as the ASME Boiler and Pressure Vessel Code, for safe use in the power generation sector.

Applications in Power Plants

Boiler Tubes: Used in the high-temperature sections of boilers to transport and superheat steam.

Superheater and Reheater Piping: Handles high-temperature, high-pressure steam to ensure efficient power generation.

High-Pressure Piping: Used for main steam and water supply lines that must withstand extreme pressure and temperature conditions.

 

Specification Of GH4080A alloy seamless tubes for power plants

 

Category Details
Introduction GH4080A is a nickel-chromium-based superalloy that exhibits good strength at high temperatures along with excellent corrosion resistance and oxidation resistance. These advantages make 4080A widely used in high-temperature forged components in aerospace, power generation, and transportation industries.
Chemical Composition (%) Element Min Max  
  Nickel (Ni) Balance Balance  
  Chromium (Cr) 18.00 21.00  
  Iron (Fe) - -  
  Molybdenum (Mo) - -  
  Carbon (C) - 0.10  
  Copper (Cu) - -  
  Aluminum (Al) 1.00 1.80  
  Manganese (Mn) - -  
  Sulfur (S) - 0.012  
  Silicon (Si) - 1.00  
  Titanium (Ti) 0.30 0.70  
  Phosphorus (P) - -  
  Tungsten (W) - -  
Physical Properties Density: 8.19 g/cm³
  Melting Point: 1320-1365°C
Applications Aero-engine combustion chamber flame tubes, afterburner casings, adjustable flaps, structural components of gas turbine combustion chambers, turbo-engine combustion chamber parts, afterburner components.

 

GH4080A alloy seamless tubes for power plants Specification

 

GH4080A Chemical Composition (wt.%)

Element Min (%) Max (%)
C 0.04 0.10
Si - 0.80
Mn - 0.40
P - 0.020
S - 0.015
Cr 18.00 21.00
Ni Bal Bal
Mo - -
V - -
Ta - -
W - -
N - -
Cu - 0.200
Co - 2.00
Pb - -
B - 0.008
Nb - -
Al 1.00 1.80
Ti 1.80 2.70
Other - -

 

GH4080A Physical Properties

Property Value Range Unit
Tensile Strength 115-234 MPa
Yield Strength 23 MPa
Elongation 65 %
Reduction of Area (ψ) - %
Impact Energy (Akv) - J
Brinell Hardness (HBS) 123-321 -
Rockwell Hardness (HRC) 30 -

 

Grade High Temperature Gh3044
Standard ASTM B704 / ASTM B704
Range 1/2″ Nominal Bore To 16″Nominal Bore
Length Single Random, Double Random & Cut Length.
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Round, Square, Rectangular, Hydraulic Etc
Type Seamless / ERW / Welded / Fabricated / EFW
Applications Off-Shore Oil Drilling Companies, Power Generation, Petrochemicals, Gas Processing, Specialty Chemicals, Pharmaceuticals, Pharmaceutical Equipment, Chemical Equipment, Sea Water Equipment, Heat Exchangers, Condensers, Pulp and Paper Industry

 

GH4080A alloy seamless tubes for power plants Surface Treatments

  • Pickling treatment
    Gnee Steel
    Pickling treatment
  • Mirror polishing treatment
    Gnee Steel
    Mirror polishing treatment
  • Polishing treatment
    Gnee Steel
    Polishing treatment
  • Sandblasting treatment
    Gnee Steel
    Sandblasting treatment

Gnee Steel provides four surface treatments for GH4080A alloy seamless tubes for power plants: pickling, mirror polishing, polishing, and sandblasting.

 

GH4080A alloy seamless tubes for power plants production process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel provides the following heat treatments for GH4080A alloy seamless tubes for power plants: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

GH4080A alloy seamless tubes for power plants Packaging 

  • Steel strapping
    Gnee Steel
    Steel strapping
  • Wooden boxes/crates
    Gnee Steel
    Wooden boxes/crates
  • Rainproof cloth packaging
    Gnee Steel
    Rainproof cloth packaging
  • Airworthy export packaging 

     

     

    Gnee Steel
    Airworthy export packaging 

In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.

 

 

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Hot Tags: gh4080a alloy seamless tubes for power plants, China gh4080a alloy seamless tubes for power plants suppliers, alloy margin, alloy component, alloy event, alloy optimization, alloy benchmark, alloy advertising

Send Inquiry

whatsapp

Phone

E-mail

Inquiry