GH2132 Alloy Rods For High-temperature Furnaces
Specification: GB/T 14994
Grade: GH2132
Length: Customized
Round Bar Diameter: 4.00 mm to 400 mm
Bright Bar: 4 mm to 150 mm
Surface Treatment: Black, Bright, Polished
Shapes: Round Bars, Billets, Ingots, Forgings, etc.
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
GH2132 alloy rods for high-temperature furnaces description

GNEE GH2132 alloy rods for high-temperature furnaces
GH2132 (also known as A-286 or UNS S66286) is an iron-nickel-chromium-based superalloy bar designed for applications requiring high strength, oxidation resistance, and creep resistance at high temperatures. It is a versatile high-temperature material used in the manufacture of components for industrial furnaces.
GH2132 is our main production grade, and it has gained recognition from customers in numerous countries since production began. Our products include GH2132 round bars, flat bars, forgings, as well as professionally high-precision machined fasteners, shafts, washers, screws, studs, nuts, bolts, OEM parts, and custom-machined parts. Delivery conditions include quenched and tempered, annealed, and machined semi-finished products. We strictly manage packaging to avoid material damage during transportation. Gnee Steel is the best supplier of GH2132 material and is willing to develop together with customers worldwide.
Specification Of GH2132 alloy rods for high-temperature furnaces
| Grade | GH2132 |
| Standard | ASTM B463 / ASME SB463 |
| Thickness | 0.1mm To 100 mm |
| Size | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Form | Sheets, Plates, Coils, Slatting Coils, Perforated Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
| Applications | Off-Shore Oil Drilling Companies, Power Generation, Petrochemicals, Gas Processing, Specialty Chemicals, Pharmaceuticals, Pharmaceutical Equipment, Chemical Equipment, Sea Water Equipment, Heat Exchangers, Condensers, Pulp and Paper Industry |
GH2132 alloy rods for high-temperature furnaces Specification
GH2132 rods Chemical Composition (Weight %)
| Element | Minimum | Maximum |
|---|---|---|
| Nickel (Ni) | 24.0 | 27.0 |
| Chromium (Cr) | 13.5 | 16.0 |
| Iron (Fe) | Balance | Balance |
| Boron (B) | 0.003 | 0.010 |
| Molybdenum (Mo) | 1.0 | 1.5 |
| Vanadium (V) | 0.1 | 0.5 |
| Carbon (C) | - | 0.08 |
| Manganese (Mn) | - | 0.35 |
| Silicon (Si) | - | 0.35 |
| Sulfur (S) | - | 0.002 |
| Phosphorus (P) | - | 0.015 |
| Copper (Cu) | - | 0.3 |
| Aluminum (Al) | 1.9 | 0.35 |
| Titanium (Ti) | - | 2.35 |
GH2132 Bar Physical Properties
| Property | Value | Conditions / Notes |
|---|---|---|
| Density | 7.99 g/cm³ | |
| Melting Point | 1364 - 1424 °C | |
| Thermal Conductivity (λ) | 14.2 W/(m·°C) | At 100°C |
| Specific Heat Capacity | - | Data not provided |
| Elastic Modulus | - | Data not provided |
| Shear Modulus | - | Data not provided |
| Resistivity | 0.914 μΩ·m | |
| Linear Expansion Coefficient (a) | 15.7 x 10⁻⁶ /°C | From 20°C to 100°C |
GH2132 rods Mechanical Properties (Solution State)
| Property | Value |
|---|---|
| Tensile Strength (σb) | 930 MPa |
| Yield Strength (RP0.2) | 590 MPa |
| Elongation (A) | > 15 % |
| Brinell Hardness (HB) | ≤ 341 |
application Of GH2132 alloy rods for high-temperature furnaces
High-Temperature Furnace Applications
GH2132 alloy bars are suitable for industrial furnaces, heat treatment equipment, and other heat treatment systems, especially in applications requiring the withstand of significant thermal and mechanical stresses. Specific applications include:
Structural Components: The bars can be used for furnace support structures, connectors, and internal clamps.
Heating Element Supports: This alloy exhibits excellent stability and strength at high temperatures, making it suitable for supporting heating elements and protecting them from corrosive gases and materials.
Heat Exchangers: Heat exchanger assemblies used in high-temperature environments.
GH2132 alloy rods for high-temperature furnaces production process
Gnee Steel provides the following heat treatments for GH2132 alloy rods for high-temperature furnaces: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.
GH2132 alloy rods for high-temperature furnaces Packaging
1. Packaging is crucial, especially in international shipping, where goods undergo multiple stages to reach their final destination; therefore, we place great emphasis on packaging.
2. Gnee Steel employs various packaging methods depending on the product. For example, we use multiple packaging methods...

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.
Hot Tags: gh2132 alloy rods for high-temperature furnaces, China gh2132 alloy rods for high-temperature furnaces suppliers, alloy alternative, alloy characteristic, dispersion strengthening alloy, virgin alloy, alloy benchmark, alloy shortage
You Might Also Like
Send Inquiry