1J50 is a nickel-iron magnetic alloy with approximately 50% nickel and 48% iron. It is based on permalloy. It has the characteristics of high magnetic permeability and high saturation magnetic flux density.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
super alloy Products Application

1J50 3J40 Steel Alloy Pipe video

This combination alloy is mainly used for aviation elastic components that require wear resistance, corrosion resistance, shock resistance, non-magnetic, and high strength, such as shaft tips, tension wires, hairsprings, springs, springs, and diaphragms; it is also used to make components with high requirements. Corrosion-resistant, non-magnetic special bearings, small shafts, balls, stamping dies and cutting tools, etc.

super alloy Material Specification

 

Alloy

C

P

S

Si

Mn

Ni

Cr

Mo

Ti

Zr

Al

Ce

Ca

Fe

Max

 

3J40

0.03

0.01

0.01

0.2

0.1

REST

39-41

–

–

–

3.3-3.5

Trace

–

<0.5

1J50 3J40 Steel Alloy Pipe

1J50 3J40 Steel Alloy Pipe video1J50 3J40 Steel Alloy Pipe video

1J50 iron-nickel soft magnetic alloy is a soft magnetic alloy with high magnetic permeability, low remanence and coercivity. In its standard ingredient formula, Fe and Ni each account for about 50%. Because this type of alloy has a narrow and steep hysteresis loop, a large magnetic permeability and a small coercive force in a weak magnetic field, it is widely used in transformers, magnetic shields, magnetic heads, aerospace precision control instruments and other fields. widely used. In addition, 1J50 alloy has good processing performance and can be made into various components with complex shapes and precise dimensions. Therefore, it is often used as precision magnetic components in the aerospace field.

High hardness, high strength, non-magnetic, corrosion-resistant and highly elastic alloy 3J40 is a precipitation-strengthened nickel-based alloy. It has good plasticity in the solid solution state and is easy to process. It obtains high mechanical properties and elastic properties after large strain rate cold working and aging treatment. . The alloy can also be strengthened by aging after solid solution. 3J40 is a Ni-Cr-Al alloy with a chromium content of up to 40% and excellent corrosion resistance.

Customer Case

 

 

customer visit

1J50 3J40 Steel Alloy Pipe video

1J50 3J40 Steel Alloy Pipe video

FAQ

 

 

 

 

 

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.

Q: About the product price of 1J50 3J40 Steel Alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: 1J50 3J40 Steel Alloy Pipe, China 1J50 3J40 Steel Alloy Pipe suppliers, alloy quota, GH4169 nickel alloy, alloy satisfaction, 2 4669 stainless steel plate, alloy marketing, alloy price

Send Inquiry

whatsapp

Phone

E-mail

Inquiry