What Is The Temperature Limit For Inconel 600?

What is the temperature limit for Inconel 600?

 

 

Description
Alloy 600 is a non-magnetic nickel-based high temperature alloy that exhibits excellent properties such as high strength, hot and cold workability, and resistance to general corrosion.
The alloy also exhibits good heat resistance and will not age or develop stress corrosion in the annealed to heavily cold worked condition.

What is the temperature limit for Inconel 600?What is the temperature limit for Inconel 600?

Applications
Some typical applications include:

Barge and tank car linings
Carburizing atmospheres
Ethylene chloride cracking furnaces
Heat plates, mufflers, hangers
Gasoline stabilizer production
MgCl2 evaporators
Phenol condensers
Soap manufacturing
Titanium dioxide
Vegetable and fatty acid containers
Corrosion resistance
The high chromium content of Alloy 600 makes it much more resistant to oxidation than pure nickel, while its high nickel content provides good corrosion resistance under reducing conditions.
The alloy exhibits high resistance to stress and brines, exhaust gases, and most organic acids and compounds.

Heat Treatment
Alloy 600 is not an age-hardenable alloy; cold working is the only available hardening method. Annealing softening begins at about 1600°F (871°C) and is essentially complete after heating at 1800°F (982°C) for 10 to 15 minutes. Above this temperature, grain growth may be objectionable, but very brief heating at 1900°F results in complete softening without excessive grain growth. Since the cooling rate has no effect on softening, the material can be water quenched or air cooled.

Machinability
Hot Working/Forging
A low-sulfur reducing furnace atmosphere should be used for forging. Major hot working should be performed between 2300/1850°F, while light working may be continued at temperatures as low as 1600°F. Hot working should not be attempted between 1600/1200°F because of the lower ductility in this range.

Machinability
Alloy 600 can be machined in both the hot-worked and annealed conditions. Because machining this alloy generates considerable heat, high-speed steel, cast nonferrous, or carbide tools should be used. Tools should be kept sharp.
Lathe turning speeds are 35/45 sfm (0.18/0.23 m/s) with high-speed and nonferrous tools; 100/175 sfm (0.51/0.89 m/s) with carbide tools. (This data should be used as a guide only for initial machine settings. The figures used are averages. The nature of the part may require adjustment of speeds and feeds in some jobs.)
Sulfur-containing oils should be used as lubricants but should be completely removed before exposing machined parts to high temperatures (such as welding).

Cold Working
For improved properties, Alloy 600 can be cold worked to temperatures below 1200°F (649°C).

Welding
Alloy 600 can be joined by common welding, brazing, and soldering processes.