What Is The Maximum Temperature For Incoloy 800H?

What is the maximum temperature for incoloy 800H?

 

Incoloy 800H/800HT Plate – High Strength Nickel Alloy for Extreme Temperatures
Gnee Steel is a supplier of Incoloy 800H/800HT nickel alloy. The nickel-iron-chromium alloy is designed to resist oxidation and carburization and has higher creep and stress rupture properties than 800 alloy (UNS N08800).

Available thicknesses for Incoloy alloy 800H/800HT:

3/16" 1/4" 3/8" 1/2" 5/8" 3/4"
4.8mm 6.3mm 9.5mm 12.7mm 15.9mm 19mm
1" 1 1/4" 1 1/2" 1 3/4" 2"  
25.4mm 31.8mm 38.1mm 44.5mm 50.8mm

What is the maximum temperature for incoloy 800H?What is the maximum temperature for incoloy 800H?

General Properties
Incoloy 800H alloy (UNS N08810) and 800HT alloy (UNS N08811) are dual certified nickel-iron-chromium alloy materials that resist oxidation, carburization, and other high temperature corrosion properties. These nickel alloys have the same chemical composition as Incoloy 800 alloy (UNS N08800), but with higher carbon contents: 0.05-0.10% for Incoloy 800H alloy and 0.06-0.10% for Incoloy 800HT alloy. Incoloy 800HT alloy also has additions of up to 1.0% aluminum and titanium. In addition to the chemical composition restrictions, both alloys are high temperature annealed to an average grain size of ASTM 5 or coarser. The stringent chemical composition and high temperature annealing process ensure that these materials have higher creep and rupture strengths than Incoloy 800 alloy.

Incoloy 800H alloy has good creep rupture properties at temperatures above 600°C (1100°F). Due to the titanium and aluminum contents up to 0.7%, good ductility is maintained even for long-term use at temperatures below 700°C (1290°F). Standard annealing of Incoloy 800 alloy is recommended for use at temperatures below 600°C (1100°F). Incoloy 800H alloy resists reducing, oxidizing and nitriding atmospheres, as well as alternating reducing and oxidizing atmospheres. This nickel alloy remains stable in long-term high-temperature use.

Incoloy 800HT alloy has excellent creep strength at temperatures above 700°C (1290°F). If the application involves frequent temperature swings to below 1290°F (700°C), or if the parts are exposed to temperatures below 1290°F (700°C) for long periods of time, Incoloy 800H alloy should be used. Incoloy 800HT alloy has high temperature properties comparable to Incoloy 800H alloy and is also stable in long-term high temperature service.

Incoloy 800H and 800HT alloys are readily weldable and can be processed according to standard shop fabrication practices.

Applications
Chemical and petrochemical processing – process equipment for the production of ethylene, ethylene dichloride, acetic anhydride, ethylene ketone, nitric acid and oxyalcohols
Petroleum refining – steam/hydrocarbon reforming units and hydrodealkylation units
Power generation – steam superheaters and high temperature heat exchangers in gas-cooled nuclear reactors, and heat exchangers and piping systems in coal-fired power plants
Heat treatment equipment – ​​radiant tubes, muffle furnaces, stills and equipment for heat treatment furnaces

Chemical Analysis

Weight % (all values are maximum unless a range is otherwise indicated)

Element 800H 800HT
Nickel 30.0 min.-35.0 max. 30.0 min.-35.0 max.
Chromium 19.0 min.-23.0 max. 19.0 min.-23.0 max.
Iron 39.5 39.5
Carbon 0.05 min.-0.10 max. 0.06 min.-0.10 max.
Manganese 1.50 1.50
Phosphorus 0.045 0.045
Sulfur 0.015 0.015
Silicon 1.0 1.0
Aluminum 0.15 min.-0.60 max. 0.25 min.-0.60 max.
Titanium 0.15 min.-0.60 max. 0.25 min.-0.60 max.
Aluminum & Titanium 0.30 min.-1.20 max. 0.85 min.-1.20 max.