4140 Alloy Steel Forged Bar
video

4140 Alloy Steel Forged Bar

Alloy: 4140 HR HT
Diameter: 6.500 inches
Cutting tolerance: 0.125 inches/-0 inches.
Cutting size range: 0.375 inches to 72 inches in 0.125 inch increments.
For sizes and tolerances outside this range, please contact us.
Typical Mechanical Properties
Brinell Hardness – 269/341BHN
Tensile Strength – 156,000 PSI
Yield Strength – 123,500 PSI
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

4140 Steel Forged Bar introduce

4140 Alloy Steel Forged Bar

What material is Inconel600 and what is the implementation standard

 

Gnee Steel 4140 Alloy Steel Forged Bar

Gnee Steel distributes premium AISI 4140 alloy steel forged bars and forgings. Our stock is available for immediate sawing, cutting and delivery under API Q1 and ISO 9001:2015 certified quality management system requirements.
We meet the stringent requirements of our customers with short lead times and fast turnaround.
4140 Forged Bar Features
AISI/SAE 4140 alloy steel is a low alloy steel in the chromium-molybdenum family. AISI 4140 has high strength, hardenability, good toughness, low quenching distortion, high creep strength and high temperature rupture strength. AISI 4140 alloy steel bars have a higher carbon content than AISI 4130, resulting in higher strength and heat treatability.
4140 alloy steel forged bars have a wide range of uses in the aerospace, oil and gas, and automotive industries, and are often used in downhole tools.

 

 

 

4140 Alloy Forged Bar Specification

AISI 4140 Forged Bar Mechanical Properties & Processing

Property

As-Forged

Q&T Treated

Performance Gain

Tensile Strength (MPa)

650 - 800

950 - 1200

↑46%

Yield Strength (MPa)

≥ 400

≥ 720

↑80%

Impact Toughness (J)

50 - 65

35 - 45

↓30%

Fatigue Limit (MPa)

240

380

↑58%

Forging Temp Range

1150-850°C (Hammer/Die)

-

Optimal grain refinement

Standard "4140 Grade" Chemical Composition

Carbon 0.38-0.43
Manganese 0.75-1.00
Phosphorus (max) 0.035
Sulfur (max) 0.040
Silicon 0.15-0.35
Chromium 0.80-1.10
Molybdenum 0.15-0.25

Estimated Mechanical Property Ranges for "Grade 4140"

Tensile strength (psi) 95,000 - 105,000
Yield strength (psi) 65,000 - 75,000
Elongation in 2" (%) 20 - 30
Reduction of area (%) 35 - 45
Brinell Hardness (BHN) 200 - 230

4140 Alloy Steel Bar Schedule 

Rounds (Inches)

1/2 1-7/8 3-1/2 6-1/4 9 14
5/8 2 3-3/4 6-1/2 9-1/2 16
3/4 2-1/8 4 6-3/4 9-3/4  
7/8 2-1/4 4-1/4 7 10  
1 2-3/8 4-1/2 7-1/4 10-1/2  
1-1/8 2-1/2 4-3/4 7-1/2 11  
1-1/4 2-5/8 5 7-3/4 11-1/4  
1-3/8 2-3/4 5-1/4 8 11-1/2  
1-1/2 2-7/8 5-1/2 8-1/4 12  
1-5/8 3 5-3/4 8-1/2 13  
1-3/4 3-1/4 6 8-3/4 13-1/2  

Squares (Inches)

1/2 1 1-3/4 3-1/2 6
5/8 1-1/8 2 4  
3/4 1-1/4 2-1/2 4-1/2  
7/8 1-1/2 3 5  

Flats (inches)

1/4 x 1 3/8 x 4 5/8 x 3 1 x 2-1/2 1-1/2 x 2-1/2 2-1/2 x 3-1/2
1/4 x 1-1/2 1/2 x 1 3/4 x 1-1/2 1 x 3 1-1/2 x 3 2-1/2 x 4
1/4 x 2 1/2 x 1-1/2 3/4 x 2 1 x 4 1-1/2 x 4 2-1/2 x 6
1/4 x 3 1/2 x 2 3/4 x 2-1/2 1 x 5 1-1/2 x 5 3 x 4
1/4 x 4 1/2 x 2-1/2 3/4 x 3 1 x 6 1-1/2 x 6 3 x 5
1/4 x 5 1/2 x 3 3/4 x 4 1-1/4 x 2 2 x 2-1/2 3 x 6
1/4 x 6 1/2 x 3-1/2 3/4 x 5 1-1/4 x 2-1/2 2 x 3  
3/8 x 1-1/2 1/2 x 4 3/4 x 6 1-1/4 x 3 2 x 3-1/2  
3/8 x 2 1/2 x 5 1 x 1-1/4 1-1/4 x 3-1/2 2 x 4  
3/8 x 2-1/2 1/2 x 6 1 x 1-1/2 1-1/4 x 4 2 x 5  
3/8 x 3 5/8 x 2 1 x 2 1-1/2 x 2 2 x 6  

We stock AISI 4140 and AISI 4130 steel in round, square and flat bar. All material is hot rolled with a surface finish. Please call or email us for a free quote. Material is quenched and tempered, stress relieved and mechanically straightened. We stock a wide variety of uncommon sizes and lengths including (10/12 foot random lengths, 20/24 foot random lengths and custom cut to length options). 4140 and 4150 alloys are widely used in general purpose mechanical applications. Typically, 4150 and 4140 round bars over 10 inches in diameter are supplied in rough turned oversize.

 

4140 Steel Bar Packaging & Testing

GNEE Group 4140 Alloy Bar Packaging & Testing

 
GNEE Group 4140 Alloy Bar Packaging
GNEE Group 4140 Alloy Bar Packaging
GNEE Group 4140 Alloy Bar Testing
GNEE Group 4140 Alloy Bar Testing

Hot Tags: 4140 alloy steel forged bar, China 4140 alloy steel forged bar suppliers, toughness alloy, alloy competitor, alloy purchaser, alloy shortage, GH3030 pipe, alloy business

Send Inquiry

whatsapp

Phone

E-mail

Inquiry