4140 Seamless Steel Round Tubing introduce
4140 Alloy Seamless Round Tubing

AISI 4140 grade steel is a low alloy steel that has chromium, molybdenum and manganese added to its alloy. Compared to 4130 grade steel, 4140 grade steel has a slightly higher carbon content. This versatile alloy gives AISI 4140 pipes good properties. For example, they have good atmospheric corrosion resistance and reasonable strength.
The chemical properties of 4140 grade seamless pipes reflect good comprehensive properties such as toughness, strength, fatigue strength and wear resistance. In order to improve the mechanical properties of the parts, they need to be heat treated. In addition, the alloy has self-scaling properties, which is an important feature of 4140 alloy steel pipes. The anti-scaling property can effectively reduce the cost of processing. AISI 4140 steel pipe is considered a mechanical pipe and is produced by cold working or hot working processes, usually ingot casting or continuous casting as required. After the pipe is hot worked, it can be cold worked and finally oiled before forming. Applying oil to the surface of ASTM A519 4140 grade pipe can effectively prevent dust accumulation.
Alloy Steel Grade 4140 Pipe Sizes
| O.D. * Thk. | O.D. * Thk. | O.D. * Thk. |
|---|---|---|
| 57 * 4.9 | 38.1 * 3.2 | 76.2 * 4 |
| 57 * 6.3 | 38.1 * 4 | 76.2 * 5 |
| 57 * 7.9 | 38.1 * 6.3 | 76.2 * 6.3 |
| 60.3 * 3.2 | 42.4 * 3.2 | 82.5 * 4.5 |
| 60.3 * 3.6 | 42.4 * 4 | 88.9 * 3.2 |
| 60.3 * 5 | 44.5 * 3.2 | 88.9 * 3.6 |
| 63.5 * 3.2 | 44.5 * 6.3 | 88.9 * 4 |
| 63.5 * 3.6 | 48.3 * 3.2 | 101.6 * 3.6 |
| 63.5 * 4 | 48.3 * 3.6 | 101.6 * 4.5 |
| 63.5 * 6.3 | 50.8 * 4.5 | 101.6 * 6.3 |
| 63.5 * 7.9 | 51 * 3.2 | 114.3 * 3.6 |
| 70 * 3.2 | 51 * 3.6 | 114.3 * 5 |
| 70 * 3.6 | 51 * 6.3 | 139.7 * 4 |
| 70 * 6.3 | 57 * 3.2 | 139.7 * 5 |
| 76.2 * 3.6 | 57 * 3.6 | 139.7 * 6.3 |
4140 Seamless Round Tubing Specification
Chemical Structure of AISI 4140 Seamless Pipe
| Element | Content (%) |
|---|---|
| Iron, Fe | 96.785 - 97.77 |
| Chromium, Cr | 0.80 - 1.10 |
| Manganese, Mn | 0.75 - 1.0 |
| Carbon, C | 0.380 - 0.430 |
| Silicon, Si | 0.15 - 0.30 |
| Molybdenum, Mo | 0.15 - 0.25 |
| Sulfur, S | 0.040 |
| Phosphorous, P | 0.035 |
4140 Chrome Moly Steel Pipe Mechanical Properties
| Properties | Metric | Imperial |
| Hardness, Vickers (converted from Brinell hardness) | 207 | 207 |
| Tensile strength | 655 MPa | 95000 psi |
| Bulk modulus (typical for steel) | 140 GPa | 20300 ksi |
| Yield strength | 415 MPa | 60200 psi |
| Hardness, Rockwell C (converted from Brinell hardness. Value below normal HRC range, for comparison purposes only) |
13 | 13 |
| Elastic modulus | 190-210 GPa | 27557-30458 ksi |
| Poisson's ratio | 0.27-0.30 | 0.27-0.30 |
| Elongation at break (in 50 mm) | 25.70% | 25.70% |
| Shear modulus (typical for steel) | 80 GPa | 11600 ksi |
| Hardness, Brinell | 197 | 197 |
| Machinability (based on AISI 1212 as 100 machinability) | 65 | 65 |
| Hardness, Rockwell B (converted from Brinell hardness) | 92 | 92 |
| Hardness, Knoop (converted from Brinell hardness) | 219 | 219 |
4140 Alloy ss Steel Round Tubing Surface Treatments
Gnee Steel provides four surface treatments for Inconel ASTM B163 718 Alloy seamless Pipe: pickling, mirror polishing, polishing, and sandblasting.
4140 Alloy ss Round Tubing Packaging & testing
GNEE Group 4140 ss Round Tubing Packaging & testing


Hot Tags: 4140 alloy seamless steel round tubing, China 4140 alloy seamless steel round tubing suppliers, power generation alloy, alloy wholesaler, alloy billet, Heat Resistant Steel, alloy supply, alloy manufacturing
You Might Also Like
Send Inquiry