4130 Alloy Structural Steel Pipe
Outside Diameter: 1/2 -1-1/2"
Wall Thickness: .065 - .120"
Length:upto 288"
Schedule: 5 to 80S
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
GNEE 4130 Alloy Structural Steel Pipe introduce
4130 Structural Steel Pipe


4130 Chrome Moly Steel Pipe is a type of steel pipe made from low alloy steel containing chromium and molybdenum. It is also known as Chrome Moly Steel Pipe or Chrome Moly Steel Pipe.
4130 alloy pipe is known for its excellent strength-to-weight ratio and high temperature resistance. It is often used in applications that require high strength and light weight, such as the aerospace and motorsports industries.
4130 Chrome Moly Steel Pipe is also commonly used in the manufacture of bicycle frames, roll cages, and firearms components. It can be welded and formed into a variety of shapes, making it a versatile material with a wide range of uses.
In addition to its strength and high temperature resistance, 4130 Chrome Moly Steel Pipe also has good ductility and toughness, making it less susceptible to cracking and deformation. It also has excellent corrosion resistance, making it suitable for harsh environments.
Overall, 4130 alloy pipe is a high-quality and durable material that is widely used in a variety of applications that require strength, high temperature resistance, and light weight.
4130 alloy seamless round pipe is ideal for structural applications because of its high strength and higher hardness. If this low alloy steel is manufactured to ASTM A519 specifications, it can be hot finished or cold finished. If ASTM A519 Grade 4130 Pipe is used for mechanical tubing, it can be made by continuous casting or ingot casting. The steel is usually processed in the hot state to make 4130 alloy steel seamless pipe. If necessary, these hot-worked pipes are then cold finished to bring them to the appropriate size, shape or properties. Pipes are usually sold in the following shapes: square, round, rectangular and specific cross-sections. Thermal analysis can be used to narrow down the selection of a specified element. Before any shaping process is performed on the 4130 Chrome Molybdenum Steel Pipe, a thin layer of oil can be applied. If the buyer wants to prevent the pipe from rusting, it can be coated.
GNEE Alloy 4130 Structural Pipe Specification Sheet
4130 Chromoly Tubing Specification
| Specifications | ASTM A29 ASME SA29 |
| Dimensions | ASTM, ASME and API |
| Size | 4 to 219mm W. T.: 0.5 to 20mm |
| Specialized in | Large Diameter Size |
| Length | Within 13500mm |
| Type | Seamless / ERW / Welded / Fabricated |
| Form | Round, Hydraulic Etc |
| Length | Single Random, Double Random & Cut Length. |
| End | Plain End, Beveled End, Treaded |
4130 Pipes Chemical Composition
| Element | Content (%) |
|---|---|
| Iron, Fe | 97.03 – 98.22 |
| Chromium, Cr | 0.80 – 1.10 |
| Manganese, Mn | 0.40 – 0.60 |
| Carbon, C | 0.280 – 0.330 |
| Silicon, Si | 0.15 – 0.30 |
| Molybdenum, Mo | 0.15 – 0.25 |
| Sulfur, S | 0.040 |
| Phosphorous, P | 0.035 |
GNEE 4130 Structural Pipe Schedule
AISI 4130 Seamless Pipe Sizes in Stock
| Pipe Form | Size Range | Thickness | Dimension Standards |
|---|---|---|---|
| 4130 Steel Seamless Pipe | 1/8" to 16" inches | Sch 5, 5s, 10, 10s, 20, 30, 40s, 40, STD, 60, 80s, 100, 120, XS, XXS, 160 | ANSI B36.10, ANSI B36.19, ANSI B36.19M |
SAE AISI 4130 Welded Pipe Size Chart
| Size | ID | OD | Wall Thickness |
|---|---|---|---|
| 1 | 1.049 | 1.315 | 0.133 |
| 3/4 | 0.824 | 1.05 | 0.113 |
| 1 1/4 | 1.380 | 1.66 | 0.140 |
| 2 | 2.157 | 2.375 | 0.109 |
| 1 1/2 | 1.610 | 1.90 | 0.145 |
| 2 1/2 | 2.635 | 2.875 | 0.120 |
| 1/2 | 0.622 | 0.84 | 0.109 |
| 3 1/2 | 3.760 | 4.0 | 0.120 |
| 3 | 3.260 | 3.50 | 0.120 |
| 4 | 4.260 | 4.5 | 0.120 |
| 6 | 6.407 | 6.625 | 0.109 |
| 5 | 5.187 | 5.563 | 0.188 |
GNEE Group Factory Environment
GNEE Group 4130 Alloy Steel Pipe Factory Environment

GNEE Group 4130 Pipe Packaging
GNEE Group 4130 Steel Pipe Packaging

GNEE Group Testing
GNEE Group 4130 Alloy Pipe Testing

FAQ
1. What is 4130 chrome-molybdenum steel used for?
4130 chrome-molybdenum steel (Chromoly) cold-drawn seamless round tube is one of the most widely used steel tubes in the manufacture of racing chassis and roll cages. Its excellent strength-to-weight ratio has been the preferred choice of racing car and aircraft manufacturers since the early 20th century.
2. Is chrome-molybdenum steel better than steel?
What distinguishes chrome-molybdenum steel from other types of steel is its higher tensile strength. This means it can withstand greater forces without breaking or deforming. It also has better corrosion resistance, making it ideal for applications exposed to harsh environments or moisture.
3. Will 4130 chrome-molybdenum steel rust?
Both 4140 and 4130 steels are low-alloy steels that have excellent strength, toughness, and corrosion resistance.
4. Is 4130 a carbon steel?
4130 carbon steel is a low-carbon steel with a carbon content of approximately 0.3%. 4130 is also an alloy steel with chromium and molybdenum as strengthening agents. This steel is easy to weld and can be heat treated more easily than other mild steels.
Hot Tags: 4130 alloy structural steel pipe, China 4130 alloy structural steel pipe suppliers, machining alloy, alloy quota, thermal expansion alloy, alloy end user, GH4169 alloy, alloy wholesaler
You Might Also Like
Send Inquiry