What Non-Grain-Oriented Silicon Steel Is
Non-grain-oriented silicon steel, usually abbreviated as non-oriented electrical steel, is a low-carbon iron-silicon alloy supplied as cold-rolled strip and sheet in which the crystal grains are randomly oriented after the final deformation and annealing cycle. Because there is no preferred grain direction, the magnetic properties are almost the same along the rolling direction and across it, which is exactly what a rotating machine needs. The material is the standard core material for motors, generators, small transformers, welding transformers, ballasts and reactors.
Chemistry and Why Silicon Is Added
The alloy is essentially iron with a controlled silicon addition and a very low carbon level.
| Element | Typical content | Function |
|---|---|---|
| Silicon | A few percent, commonly within roughly 1–3.5 wt% | Raises electrical resistivity, which suppresses eddy current losses, and reduces magnetostriction and hysteresis loss |
| Carbon | Held very low, typically below 0.01 wt% | Prevents magnetic aging; residual carbon raises hysteresis loss over time |
| Aluminium | Small controlled additions | Further increases resistivity and helps control grain growth during annealing |
| Manganese and sulphur | Low, balanced against each other | Manganese ties up sulphur so that harmful sulphide inclusions do not pin the magnetic domain walls |
| Iron | Balance | Provides the ferromagnetic matrix |
A higher silicon content lowers losses but also lowers saturation induction and makes the strip harder and more brittle, so the grades actually produced represent a deliberate compromise between magnetic loss and mechanical workability.
How Cold-Rolled Non-Oriented Strip Is Produced
Production starts with hot-rolled coil or continuously cast slab. The material is hot rolled to a transfer thickness of roughly 2–2.5 mm, pickled, then cold rolled in one or more passes down to the final gauge, which for non-oriented grades is normally 0.35 mm, 0.50 mm or 0.65 mm. After cold rolling the strip is annealed to recrystallise the structure and grow the grains, and it is finally coated with an insulating layer and slit to width. The cold-rolled route gives a flat surface, uniform thickness and a high stacking factor, together with higher magnetic induction and lower core loss than hot-rolled silicon steel strip of the same thickness. Because the cold-rolled strip is magnetically better, a designer can reach the same output with less core mass and less volume than a hot-rolled design, and the resulting machine runs at lower loss and with more predictable performance.
Grades and How to Read Them
Non-oriented grades are normally designated by strip thickness and guaranteed specific total loss, so the grade number itself carries the loss data. Under GB/T 2521.1, for example, the designation 50W600 means a nominal thickness of 0.50 mm, non-oriented grain structure, and a maximum specific total loss of 6.00 W/kg measured at 1.5 T and 50 Hz.
| Example designation | Nominal thickness | Maximum specific total loss at 1.5 T, 50 Hz | Typical use |
|---|---|---|---|
| 35W300 | 0.35 mm | 3.00 W/kg | High-efficiency motors and small transformers |
| 50W470 | 0.50 mm | 4.70 W/kg | Premium industrial motors and generators |
| 50W600 | 0.50 mm | 6.00 W/kg | General-purpose motors and compressors |
| 50W800 | 0.50 mm | 8.00 W/kg | Standard motors and small transformers |
| 65W1000 | 0.65 mm | 10.00 W/kg | Larger frames and welding transformers |
Comparable international designations exist in IEC 60404-8-4 and in EN 10106 for fully processed material, and the ASTM specifications separate fully processed types, ASTM A677, from semi-processed types, ASTM A683. Because the naming rule encodes the guaranteed loss, a buyer can compare offers by reading the grade designation rather than by trusting a general description.
Magnetic Behaviour: Random Grains and What They Cost
In grain-oriented steel the grains are aligned so that the easiest magnetisation direction follows the rolling direction, which gives very low loss in the direction of flux in a transformer core. Non-oriented steel deliberately gives that up. The random orientation produces isotropic behaviour, so flux can flow in any direction in the plane of the sheet with essentially equal permeability, which suits the rotating flux pattern of a motor stator and rotor. The trade-off is a higher core loss than a grain-oriented grade of the same thickness, and it is accepted because a motor core cannot use a single easy axis.
Permeability: substantially the same along and across the rolling direction.
Core loss: higher than grain-oriented steel, since no benefit can be taken from grain alignment.
Magnetostriction: controlled by chemistry and processing to limit acoustic noise in motors.
Punching behaviour: good, because the grade is supplied flat, uniform and with a coating that resists tool wear.
Applications
Induction and synchronous motors, including high-efficiency and inverter-fed drives.
Generators, alternators and small power generation sets.
Distribution, instrument and welding transformers, plus chokes and reactors.
Compressors, pumps and domestic appliance motors.
Electromobility traction motors, where thin, low-loss grades matter most.
Specifying and Buying Non-Oriented Steel
Loss guarantee: state the grade designation and the test condition, normally 1.5 T at 50 Hz or 60 Hz, since loss measured at 60 Hz is not interchangeable with loss at 50 Hz.
Thickness and stacking factor: thinner strip reduces eddy current loss but lowers the stacking factor of a laminated core, so the two must be balanced against the available slot area.
Surface insulation: the coating type determines whether the core can be stress-relief annealed after punching, and how well it resists inter-laminar short circuits.
Mechanical properties: yield strength and elongation matter for high-speed punching lines, and hardness matters for tool life.
Certification: request the test certificate for the actual delivered coil, since magnetic properties vary from coil to coil within a grade.
Frequently Asked Questions
Q: What does non-oriented mean in silicon steel?
It means the crystal grains in the finished strip have no preferred direction, so magnetic properties are nearly identical along, across and at an angle to the rolling direction.
Q: Why is non-oriented steel used in motors instead of grain-oriented steel?
Motor cores carry flux in rotating directions. Grain-oriented steel only performs well along one axis, so non-oriented steel gives a better overall result despite its higher basic loss figure.
Q: What silicon content is normal?
Most commercial non-oriented grades contain a few percent of silicon. Raising silicon lowers loss by increasing resistivity but reduces saturation induction and workability, so the level is a compromise set by the grade.
Q: How is the grade number related to core loss?
The number after the W is the maximum specific total loss at 1.5 T and 50 Hz expressed in units of 0.01 W/kg. A 50W600 grade therefore guarantees no more than 6.00 W/kg.
Q: What thicknesses are available?
The most common gauges are 0.35 mm, 0.50 mm and 0.65 mm, with thinner material used where low loss is critical and thicker material used where low cost and good stacking factor dominate.
Q: Does the surface coating matter?
Yes. The insulating coating limits inter-laminar eddy currents and determines whether the punched laminations can be stress-relief annealed without damaging the insulation.