Sep 25, 2025 Leave a message

Nickel 200 (UNS N02200) Flanges: Why Caustic Service Specifies Them

What Nickel 200 Is

Nickel 200, designated UNS N02200, is a commercially pure wrought nickel with a minimum nickel content of 99.0 percent. It is the simplest material in the nickel alloy family: there is no chromium, no molybdenum and no deliberate precipitation hardening addition, so its properties come from the metal itself rather than from alloy design. Carbon, manganese, iron, silicon, copper and sulphur are held to low maxima, and the resulting metal is ductile, magnetic at room temperature and highly resistant to caustic alkalies.

Product forms are covered by ASTM B160 for rod and bar, ASTM B162 for plate, sheet and strip, ASTM B161 and ASTM B163 for seamless tube and condenser tube respectively, ASTM B725 for welded pipe, and ASTM B564 for forged flanges, fittings and valves. Flanges are therefore normally produced from forged blanks under ASTM B564, machined to the dimensions of ASME B16.5 or EN 1092-1.

Composition and Property Profile

Element or property Value
Nickel, minimum 99.0 percent
Carbon, maximum 0.15 percent
Iron, maximum 0.40 percent
Manganese, maximum 0.35 percent
Silicon, maximum 0.35 percent
Copper, maximum 0.25 percent
Sulphur, maximum 0.01 percent
Density 8.89 grams per cubic centimetre
Melting range Approximately 1446 degrees Celsius
Curie temperature Approximately 360 degrees Celsius
Annealed tensile strength, minimum 379 MPa (55 ksi)
Annealed yield strength, minimum 103 MPa (15 ksi)
Annealed elongation, minimum 40 percent

Two numbers in that table matter for flange selection. The 99.0 percent minimum nickel assures the caustic resistance, and the low carbon of the related grade Nickel 201, UNS N02201, at 0.02 percent maximum, controls the graphitisation risk that appears above about 315 degrees Celsius.

Why Caustic and Reducing Environments Choose Nickel 200

Nickel 200 is the standard material for handling sodium hydroxide and potassium hydroxide, because it resists both the general corrosion and the stress corrosion cracking that attack carbon steel and stainless steel in concentrated caustic. It is also resistant to neutral and alkaline salt solutions, to reducing acids where aeration is absent, and to dry chlorine and hydrogen chloride at moderate temperature. Notable limits apply in the other direction: the alloy performs poorly in oxidising media and in strongly aerated acids, where a chromium-bearing alloy is a better choice.

In flanged joints this performance is used in caustic evaporator and concentrator circuits, in chlor-alkali plants, in fatty acid and soap processing, and in equipment that handles synthetic fibre intermediates. The flange is usually the point where a dissimilar material transition occurs, which means the corrosion risk at the joint deserves as much attention as the pipe itself.

Physical Properties Relevant to Flange Design

Pure nickel conducts heat and electricity far better than austenitic stainless steel, so a flange made from it transfers heat into the bolting and changes the temperature profile of the joint. Thermal expansion is lower than that of austenitic stainless steel, which matters in a mixed-material flanged pair: the differential expansion between a nickel flange and a stainless steel mating flange must be accounted for in the bolt pre-load and in the gasket seating calculation. The alloy is magnetic below its Curie temperature of about 360 degrees Celsius, which can rule it out in instruments or equipment where a magnetic signature is unacceptable.

Temperature Limitations and Grade Selection

Nickel 200 is used in caustic service at elevated temperature, but above about 315 degrees Celsius the low carbon grade Nickel 201 is preferred because the higher carbon of Nickel 200 can graphitise and reduce ductility at temperature. Nickel 200 is also not recommended for extended service in sulphur-bearing atmospheres at high temperature, where nickel sulphide formation causes rapid attack. For flanges that will operate above 315 degrees Celsius, the drawing should specify Nickel 201 rather than Nickel 200, and the allowable stress must be read from ASME Section II, Part D for the correct product form and temperature.

Design, Forging and Inspection Considerations

Forged flanges are produced from a controlled heat, forged to direction and then machined, with a heat number traceable through the whole route. Code design follows the dimensional standard for geometry and the allowable stress rules for thickness, so the flange rating is a function of the material allowables, not of the nominal class alone. Inspection typically includes a chemical analysis of the heat, room temperature tensile testing of a coupon from the same heat and condition, ultrasonic or liquid penetrant examination of the forging where specified, and hardness testing of the finished part. Because the alloy is soft and prone to galling, bolting faces and threads require care during assembly, and the bolts themselves are usually a higher strength nickel alloy or a coated steel rather than pure nickel.

Frequently Asked Questions

Q: What is Nickel 200 UNS N02200?
A: It is commercially pure wrought nickel with a minimum nickel content of 99.0 percent, supplied in bar, plate, tube and forging forms and used mainly for caustic and reducing duty.

Q: Which standard covers Nickel 200 flanges?
A: Forged flanges, fittings and valves are covered by ASTM B564 for UNS N02200, with the finished dimensions normally taken from ASME B16.5 or EN 1092-1.

Q: Why is Nickel 201 specified above 315 degrees Celsius?
A: Nickel 201 has a maximum carbon content of 0.02 percent against 0.15 percent for Nickel 200, which avoids the graphitisation that can reduce ductility in the higher carbon grade at temperature.

Q: Is Nickel 200 suitable for seawater service?
A: It has useful resistance in flowing seawater but is not the first choice. Where chlorides and oxidising conditions combine, a chromium and molybdenum bearing alloy gives better pitting resistance.

Q: Is the material magnetic?
A: Yes, it is ferromagnetic below a Curie temperature of about 360 degrees Celsius, which must be considered where magnetic interference is a concern.

Q: What should be checked on the material certificate?
A: The heat analysis against the ASTM B564 limits, the room temperature mechanical results, the heat number and the product form. Where the flange operates at temperature, the allowable stress reference for that heat treatment and product form should also be confirmed.