Alloy 825 (UNS N08825) Properties, Composition and Industrial Applications

Composition and Metallurgy of Alloy 825

Alloy 825, designated UNS N08825, is a nickel-iron-chromium alloy with deliberate additions of molybdenum, copper and titanium. It was the forerunner of the molybdenum-bearing nickel-iron-chromium family and remains an important material in chemical processing, pollution control equipment and heat exchangers for oil-well and natural gas gathering pipelines. The high nickel content keeps the structure austenitic and resistant to chloride stress corrosion cracking, molybdenum and copper together provide resistance to both reducing and oxidizing acids, and titanium stabilises the alloy against sensitisation during welding so that intergranular corrosion does not become a service problem.

Element Approximate content, wt %
Nickel 38.0–46.0
Chromium 19.5–23.5
Iron 22.0 minimum, balance
Molybdenum 2.5–3.5
Copper 1.5–3.0
Titanium 0.6–1.2
Carbon 0.05 maximum
Manganese 1.0 maximum
Silicon 0.5 maximum
Sulfur 0.03 maximum

Corrosion Resistance and Service Environments

The defining property of Alloy 825 is its ability to handle a wide spectrum of corrosive media rather than excelling in only one. In sulfuric acid it performs well across a broad range of concentrations and temperatures, because the molybdenum content addresses reducing conditions while the chromium and copper content addresses oxidizing conditions. The same balance gives good performance in phosphoric acid, in many organic acids, and in mixed acid streams encountered in chemical and petrochemical plants.

In chloride-bearing environments the alloy resists pitting, crevice corrosion and stress corrosion cracking, which allows it to be used for seawater cooling heat exchangers and for offshore product piping systems. In sour gas service, where hydrogen sulfide and chlorides are present together, it provides reliable resistance to sulfide stress cracking and is therefore common in piping and components for gas gathering and treatment facilities. It also tolerates high-temperature oxidation, although it is not intended as a high-strength structural alloy for the hottest combustion zones.

Mechanical and Physical Properties

Property Typical value
Tensile strength About 690 MPa (100 ksi)
Yield strength, 0.2 % offset About 310 MPa (45 ksi)
Elongation in 50 mm About 45 %
Density About 8.14 g/cm³
Melting range About 1370–1400 °C
Modulus of elasticity About 196 GPa
Recommended service temperature Up to about 550 °C

The alloy is austenitic and therefore non-magnetic in the annealed condition. It is readily cold formed and can be strengthened only by cold work, not by heat treatment, so it is normally supplied in the annealed condition for corrosion service.

Industrial Applications

Chemical and petrochemical processing equipment, including reactor vessels, piping and exchanger tubing handling acid streams.

Pollution control equipment such as scrubbers, ducting and stack components exposed to acidic flue gases.

Seawater cooling heat exchangers and offshore product piping systems.

Heat exchangers for oil-well and natural gas gathering pipelines, and piping and components in sour gas applications.

Heat exchangers, evaporators, scrubbers and immersion tubes in phosphoric acid production.

Air-cooled heat exchangers in refineries.

Fuel element dissolvers and other nuclear fuel processing equipment.

Composite steel pipe where resistance to stress cracking is required.

Food processing equipment that must resist both product acids and cleaning chemicals.

Fabrication, Welding and Product Forms

Alloy 825 is one of the easier nickel alloys to fabricate. It can be cold and hot formed, machined with conventional tooling, and welded by the common arc processes using a matching filler metal. The titanium addition controls the precipitation of chromium carbides at grain boundaries, so welded joints retain intergranular corrosion resistance without a post-weld heat treatment. Hot forming is normally carried out in the range 870–1170 °C followed by annealing, and annealing is performed at about 930–1030 °C with rapid cooling.

Common product forms include seamless pipe and tube to ASTM B423 and B163, welded pipe and tube to ASTM B424 and B704 or B705, and bar to ASTM B425, with corresponding ASME SB designations used for pressure equipment. For sour service, compliance with NACE MR0175 / ISO 15156 is normally specified alongside the mechanical and corrosion test requirements of the material standard.

Frequently Asked Questions

Q: What is Alloy 825?
Alloy 825 is a nickel-iron-chromium alloy, UNS N08825, with additions of molybdenum, copper and titanium that give it resistance to both reducing and oxidizing acids.

Q: Which acids does Alloy 825 resist?
It resists sulfuric and phosphoric acid over a wide range of concentrations and temperatures, as well as many organic acids and mixed acid streams.

Q: What are the typical mechanical properties of Alloy 825?
Tensile strength is about 690 MPa, yield strength about 310 MPa and elongation about 45 % in the annealed condition.

Q: Can Alloy 825 be used in seawater?
Yes. It resists chloride pitting, crevice corrosion and stress corrosion cracking, and is widely used for seawater cooling heat exchangers and offshore piping.

Q: What product forms and standards apply to Alloy 825?
Seamless pipe and tube to ASTM B423 and B163, welded pipe and tube to ASTM B424 and B704 or B705, and bar to ASTM B425, with corresponding ASME SB designations.

Q: What is the maximum service temperature of Alloy 825?
The alloy is generally used up to about 550 °C, where it maintains useful strength and good oxidation resistance.