Grade 5 (Ti-6Al-4V) titanium alloy forms a tenacious oxide scale (primarily TiO₂) during heating or processing, which must be removed to restore surface quality and corrosion resistance. The treatment methods are categorized into mechanical, chemical, and advanced processes, tailored to application requirements.
Mechanical Removal is the primary step for heavy oxide scale. Shot blasting or vapor blasting uses titanium or ceramic abrasives to avoid contamination; sandblasting is less recommended due to potential embedding. Turning or grinding removes the oxide layer and the underlying oxygen-contaminated zone, critical for high-integrity applications. Post-mechanical treatment usually requires light pickling to eliminate residual contaminants.
Chemical Pickling is the standard method for thorough descaling. The industry uses a hydrofluoric-nitric acid (HF-HNO₃) solution: 3–5% HF (dissolves oxide) and 15–30% HNO₃ (passivates and prevents hydrogen absorption). HF-HCl blends are avoided for Grade 5 due to high hydrogen uptake risks. Pickling time is controlled at 5–30 minutes, followed by rinsing and drying to maintain passivity.
Advanced Methods include laser cleaning, which uses nanosecond lasers to ablate oxide scale without damaging the substrate, suitable for precision components. Electrochemical polishing combines descaling with surface smoothing, ideal for medical or aerospace parts.
info-350-349info-351-348
info-351-348info-351-350
Common Delivery Conditions of Grade 5 titanium alloy align with ASTM B348 (bars), B338 (tubes), and B265 (sheets), defined by mechanical processing and heat treatment states:
Hot Worked (HW): As-rolled, forged, or extruded, with a coarse-grained structure. Used for rough machining, offering high formability and cost-effectiveness.
Cold Worked (CW): As-drawn or cold-rolled, with improved dimensional accuracy and surface finish. Suitable for precision components requiring tight tolerances.
Annealed (AN): The most common condition, processed at 700–800°C followed by air cooling. Achieves a balanced microstructure of α+β phases, optimizing strength, ductility, and toughness for general engineering use.
Solution Treated and Aged (STA): Solutionized at 920–950°C, quenched, and aged at 450–550°C. Maximizes strength and hardness for high-load aerospace and industrial applications.
Surface-Finished: Delivered with pickled, ground, polished, or shot-blasted surfaces, per customer specifications, ensuring compliance with corrosion resistance or bonding requirements.