About Hastelloy C22
Hastelloy C22 Chemical Requirements:
Chemical Requirements |
|||||||
|---|---|---|---|---|---|---|---|
|
Ni |
Cr |
Mn |
C |
Mo |
Si |
Fe |
|
|
Max |
Bal. |
22.5 |
0.50 |
0.015 |
14.5 |
0.08 |
6.0 |
|
Min |
20.0 |
12.5 |
2.0 |
||||
Hastelloy C22 Mechanical Properties Requirements:
Mechanical Property Requirements |
|||||
|---|---|---|---|---|---|
|
Ultimate Tensile |
Yield Strength (0.2% OS) |
Elong. in 2 in. (50.8mm) or 4D min., % |
R/A |
Hardness |
|
|
Min |
100 KSi |
45 KSi |
45 |
||
|
Max |
|||||
|
Min |
690 MPa |
310 MPa |
|||
|
Max |
|||||


Hastelloy C22 Uses and Applications
Hastelloy C22 is widely used in different industries around the world.
Here are the main uses of Hastelloy C22 -
Transportation materials: such as hot water, chemicals, oil, gas and sulfur, etc., for various industries.
Automotive industry: air and water flow systems and piping systems.
Sewage systems: industrial water pipes and water pipes. Heating, ventilation and air conditioning equipment.
Construction industry: structural applications and scaffolding.
Housing and buildings: water supply and exhaust pipes, water pipes and curtain rods.
About Hastelloy C22
Hastelloy C22 surface roughness. C22 sheet is non-magnetic and not easy to ignite. Hastelloy C22 is an alloy that is widely known for its use in the aerospace industry. Due to its excellent properties, Hastelloy C22 is used in applications that require excellent mechanical properties such as high tensile strength and hardness.
Hastelloy grades
Hastelloy X
Alloy 400
Alloy 600
Alloy 602CA
Alloy 718
Alloy C276
Hastelloy HR 120
Hastelloy HR 160
Hastelloy B3
Hastelloy C2000
Hastelloy C22
Hastelloy G30