NS142 NS333 Stainless Steel Mechanical Tubing
video

NS142 NS333 Stainless Steel Mechanical Tubing

NS142 alloy is a general engineering alloy that is resistant to acid and alkali metal corrosion in both oxidizing and reducing environments. The high nickel content gives the alloy effective resistance to stress corrosion cracking.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
super alloy Products Application

NS142 NS333 Stainless Steel Mechanical Tubing Video

(1) Containers for cooking and bleaching in the pulp and paper industry.

(2) Scrubber, reheater and wet steam fan in the desulfurization system.

(3) Equipment and components operating in sour gas environments

(4) Acetic acid and acid product reactor

(5) Sulfuric acid condenser

(6) Methylene diphenyl isocyanate

(7) Production and processing of impure phosphoric acid

super alloy Material Specification

 

 

%

Ni

Cr

Fe

C

Mn

Si

Cu

Mo

Al

Ti

P

S

 

Min.

38

19.5

balance

 

 

 

1.5

2.5

1.0

0.6

 

 

Max.

46

23.5

balance

0.05

1

0.5

3

3.5

0.2

1.2

0.02

0.03

NS142 NS333 Stainless Steel Mechanical Tubing

NS142 NS333 Stainless Steel Mechanical TubingNS142 NS333 Stainless Steel Mechanical Tubing

NS142 alloy is a general engineering alloy that is resistant to acid and alkali metal corrosion in both oxidizing and reducing environments. The high nickel content gives the alloy effective resistance to stress corrosion cracking. It has good corrosion resistance in various media, such as sulfuric acid, phosphoric acid, nitric acid and organic acids, alkali metals such as sodium hydroxide, potassium hydroxide and hydrochloric acid solution. The higher comprehensive performance of 825 alloy is demonstrated in nuclear combustion dissolvers with various corrosive media, such as sulfuric acid, nitric acid and sodium hydroxide, all processed in the same equipment.
NS333 is a tungsten-containing nickel-chromium-molybdenum alloy with extremely low silicon and carbon content. In the oxidized and restored state, it has excellent corrosion resistance to most corrosive media. Excellent resistance to pitting corrosion, crevice corrosion and stress corrosion cracking. NS333 alloy contains a large amount of elements such as Cr and Mo and has a single-phase austenite structure. Corrosion-resistant alloys have many excellent properties, including good oxidation resistance and moderate reductive corrosion. It has excellent resistance to stress corrosion cracking and localized wear, and has satisfactory corrosion resistance in many chemical process media, including constant strength inorganic acid solutions, chlorine and chlorine-containing media, dry chlorine, formic acid and Soaking in acetic acid, sea water, brine, etc.

Customer Case

 

 

customer visit

NS142 NS333 Stainless Steel Mechanical Tubing

NS142 NS333 Stainless Steel Mechanical Tubing

FAQ

 

 

 

 

 

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.

Q: About the product price of NS142 NS333 Stainless Steel Mechanical Tubing?
A: Due to cyclical changes in raw material prices, prices vary in different periods.