GH3044 Seamless Tubing For Turbo Engines
video

GH3044 Seamless Tubing For Turbo Engines

Grade: GH3044
Surface Treatment: 2B, 2D, BA NO(8)
Shape: Round, Square, Rectangular
Type: Seamless
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

GH3044 seamless tubing for turbo engines description

GH3044 seamless tubing for turbo engines

GNEE GH3044 seamless tubing for turbo engines

 

GH3044 is a nickel-based superalloy designed for high-temperature, high-stress applications, such as hot-end components of turbine engines. Due to its superior strength, oxidation resistance, and structural integrity, GH3044 seamless steel tubing is ideal for these components.

GH3044 is a high-temperature alloy, also known as Inconel 713C. It is a nickel-based superalloy with excellent high-temperature strength, oxidation resistance, and creep resistance. This alloy contains significant amounts of nickel, chromium, and aluminum, as well as trace amounts of other elements such as iron, cobalt, and titanium.

 

GH3044 tubing is commonly used in applications requiring high-temperature resistance, such as gas turbines, aerospace components, and industrial furnaces. These tubings can withstand temperatures up to approximately 1100°C (2012°F) while maintaining their mechanical properties.

 

Why Seamless Steel Pipes Are Crucial for Turbocharged Engines

The seamless structure of GH3044 steel pipes is crucial for turbocharged engine applications for the following reasons:

Superior Strength: Unlike welded steel pipes, seamless steel pipes have a uniform grain structure, resulting in higher overall strength and durability. Welded steel pipes have potential weak points at the weld seams.

Higher Reliability: Eliminating weld seams eliminates potential failure points under high pressure and thermal stress, thus improving the reliability of the steel pipe.

Stronger Corrosion Resistance: The absence of weld seams eliminates the risk of sensitization caused by welding, avoiding the problem of decreased material corrosion resistance.

Higher Dimensional Accuracy: Seamless steel pipes can be manufactured to more precise dimensions, which is crucial for precision equipment such as turbocharged engines.

 

Specification Of GH3044 seamless tubing for turbo engines

 

Category Details
Introduction GH3044 is a solution-strengthened nickel-based oxidation-resistant alloy. It exhibits high plasticity and moderate thermal strength below 900°C, along with excellent oxidation resistance, good stamping, and welding properties. It is suitable for manufacturing components of aero-engine main combustion chambers and afterburners, as well as heat shields and guide blades, for long-term service below 900°C.
Chemical Composition (%) Element Min Max  
  Nickel (Ni) Balance Balance  
  Chromium (Cr) 23.50 26.50  
  Iron (Fe) - 4.00  
  Molybdenum (Mo) - 1.50  
  Carbon (C) - 0.10  
  Copper (Cu) - 0.07  
  Aluminum (Al) 0.50 -  
  Manganese (Mn) - 0.50  
  Sulfur (S) - 0.013  
  Silicon (Si) - 0.80  
  Titanium (Ti) 0.30 0.70  
  Phosphorus (P) - 0.013  
  Tungsten (W) 13.00 16.00  
Physical Properties Density: 8.89 g/cm³
  Melting Point: 1352–1375°C
Applications Aero-engine combustion chamber flame tubes, afterburner casings, adjustable flaps, structural components of gas turbine combustion chambers, turbo-engine combustion chamber parts, afterburner components.

 

GH3044 seamless tubing for turbo engines Specification

 

CHEMICAL COMPOSITION OF High Temperature Gh3044 Tube:

Grade C Mn Si S Cu Fe Ni Cr
GH3044 0.10 max 0.5 max 0.80 max 0.013max - 4.0max balance 23.5 – 26.5

 

GH3044 Tube Physical Properties

Property Value Range Unit
Tensile Strength 115 - 234 MPa
Yield Strength 23 MPa
Elongation 65 %
Reduction of Area - %
Impact Energy (Akv) - J
Brinell Hardness (HBS) 123 - 321 -
Rockwell Hardness (HRC) 30 -

 

GH3044 Tube Mechanical Properties

Property Value Range Unit
Tensile Strength 231 MPa
Yield Strength 154 MPa
Elongation 56 %
Reduction of Area - %
Impact Energy (Akv) - J
Brinell Hardness (HBS) 235 - 268 -
Rockwell Hardness (HRC) 30 -

 

GH3044 Tube Heat Treatment Regime

Process
Annealing
Quenching
Tempering
Normalizing
Quenching & Tempering (Q&T)

 

Features Of GH3044 seamless tubing for turbo engines

 

product-626-452

1. High Temperature Resistance: GH3044 tube is a solid solution strengthened nickel-based alloy with excellent oxidation resistance. Below 900°C, GH3044 thin-walled tube exhibits moderate thermal strength and high ductility. Furthermore, GH3044 thin-walled tube maintains its mechanical functions stably and reliably even at extreme temperatures.

2. Oxidation Resistance: Due to the lack of a dense oxide layer, GH3044 tube exhibits a slow oxidation rate. This slow oxidation rate makes it perform well in high-temperature oxidizing environments.

3. Corrosion Resistance: The main components of this alloy include nickel, chromium, and tungsten. Even in oxidizing, reducing, or neutral environments, GH3044 tube does not corrode, making it highly suitable for a wide range of media.

4. Weldability: GH3044 tube has reliable argon arc welding and spot welding performance. In addition, GH3044 tube exhibits good resistance to stamping, seam welding, and brazing. Therefore, GH3044 pipes can be connected and repaired using basic welding/structural forming processes.

 

Applications Of GH3044 seamless tubing for turbo engines

 

product-573-492

Applications of GH3044 in Turbine Engines

GH3044 seamless steel tubing is ideal for manufacturing high-temperature components in turbine engines, including:

Exhaust manifolds and exhaust pipes: This steel tubing can withstand the extreme temperatures and pressures of exhaust gases entering the turbocharger.

Afterburner housings: In jet engine applications, this alloy is used for high-temperature components in the afterburner.

Combustion chamber linings: Can be used to manufacture combustion chamber lining components that must withstand continuous high-temperature environments.

 

GH3044 seamless tubing for turbo engines Surface Treatments

  • Pickling treatment
    Gnee Steel
    Pickling treatment
  • Mirror polishing treatment
    Gnee Steel
    Mirror polishing treatment
  • Polishing treatment
    Gnee Steel
    Polishing treatment
  • Sandblasting treatment
    Gnee Steel
    Sandblasting treatment

Gnee Steel provides four surface treatments for GH3044 seamless tubing for turbo engines: pickling, mirror polishing, polishing, and sandblasting.

 

GH3044 seamless tubing for turbo engines production process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • Solution + aging process
    Gnee Steel
    Solution + aging process

Gnee Steel provides the following heat treatments for GH3044 seamless tubing for turbo engines: annealing, solution + aging. In addition, Gnee Steel also provides hot working and cold working, which are hot rolling and cold drawing.

 

GH3044 seamless tubing for turbo engines Packaging 

  • Steel strapping
    Gnee Steel
    Steel strapping
  • Wooden boxes/crates
    Gnee Steel
    Wooden boxes/crates
  • Rainproof cloth packaging
    Gnee Steel
    Rainproof cloth packaging
  • Airworthy export packaging 

     

     

    Gnee Steel
    Airworthy export packaging 

In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.

 

 

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

FAQ

Q: Why are your GH3044 seamless steel pipes so cost-effective?

A: We eliminate intermediate links in the end-to-end production process, sourcing raw materials directly from the source.

Q: What is the minimum order quantity for GH3044 seamless steel pipes?

A: It depends on the quantity of GH3044 seamless steel pipes; there is usually no minimum order quantity limit.

Q: What is the packaging method for GH3044 seamless steel pipes?

A: Usually, we use cartons or plywood boxes for packaging, with internal protective materials to ensure the safety of the GH3044 seamless steel pipes.

Hot Tags: gh3044 seamless tubing for turbo engines, China gh3044 seamless tubing for turbo engines suppliers, alloy industry, alloy system, forming alloy, machining alloy, alloy strip, alloy market