2J52 3J21 Nickel Alloy Pipe
video

2J52 3J21 Nickel Alloy Pipe

2J52 Iron-cobalt-tungsten-molybdenum hysteresis alloy is an alloy composed of iron, cobalt, tungsten, molybdenum and other elements. It is widely used in Electronics, electrical machinery, measuring instruments and medical equipment and other fields.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
super alloy Products Application

2J52 3J21 nickel alloy Pipe video

3J21 is mainly used for aviation elastic components such as shaft tips, tension wires, hairsprings, springs, springs and diaphragms that require anti-wear, corrosion resistance, earthquake resistance, non-magnetic, and high strength below 400°C. It is also used to make products with high requirements. Corrosion-resistant, non-magnetic special bearings, small shafts, balls, stamping dies and cutting tools.

super alloy Material Specification

 

Cr Al C Fe Mn Si P S Ni Mg
Min – – – – – – – – 50.5 –
Max 0.25 0.10 0.05 Bal. 0.60 0.30 0.025 0.025 – 0.5

2J52 3J21 nickel alloy Pipe

2J52 3J21 nickel alloy Pipe2J52 3J21 nickel alloy Pipe

2J52 Iron-cobalt-tungsten-molybdenum hysteresis alloy is an alloy composed of iron, cobalt, tungsten, molybdenum and other elements. It is widely used in Electronics, electrical machinery, measuring instruments and medical equipment and other fields.
3J21 is a Co-Cr-Ni-Mo high elastic alloy. It is a deformation-strengthened cobalt-based alloy. It has good plasticity in the solid solution state and is easy to process. After high strain rate cold working and aging treatment, high mechanical properties can be obtained. performance and elastic properties. However, after solution treatment, the alloy can no longer be strengthened by aging treatment. Only after processing at a large strain rate, aging treatment can produce a strengthening effect. Density of 3J21: 8.3g/cm3 2. Performance High strength G Hardness High elastic limit G Energy storage ratio High fatigue strength Elastic hysteresis and small aftereffects Non-magnetic anti-wear Good impact resistance and excellent corrosion resistance. Can work under low and high temperature conditions, with high temperatures up to 400°C.

Customer Case

 

 

customer visit

2J52 3J21 nickel alloy Pipe

2J52 3J21 nickel alloy Pipe

FAQ

 

 

 

 

 

Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.

Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: About the product price of 2J52 3J21 nickel alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: 2j52 3j21 nickel alloy pipe, China 2j52 3j21 nickel alloy pipe suppliers, Nickel GH3030 Superalloy Pipe, solid solution strengthening alloy, ni based superalloy, value added alloy, dispersion strengthening alloy, alloy event

Send Inquiry

whatsapp

Phone

E-mail

Inquiry