Gh4049 Superalloy Bar - High Strength Nickel Alloy Rod For Aerospace, ASTM B637
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Our High-Temperature Superalloys are engineered to deliver exceptional performance in the most extreme environments. Designed for industries such as aerospace, energy, petrochemical, and industrial manufacturing, these alloys offer unmatched heat resistance, corrosion resistance, and mechanical strength. Whether you need components for gas turbines, nuclear reactors, or high-temperature furnaces, our superalloys provide the reliability and durability required for critical applications.
Key Features:
Extreme Heat Resistance: Maintains structural integrity at temperatures exceeding 1000°C.
Superior Corrosion Resistance: Resists oxidation and chemical corrosion in harsh environments.
High Mechanical Strength: Withstands heavy loads and high stress without compromising performance.
Customizable Solutions: Available in various forms, including strips, coils, rods, and bars, tailored to your specifications.
Applications:
Aerospace: Turbine blades, engine components, and structural parts.
Energy: Gas turbines, nuclear reactors, and power generation systems.
Petrochemical: Reactors, heat exchangers, and pipelines.
Industrial: High-temperature furnaces, molds, and heavy machinery.
Technical Specifications:
| Property | Typical Value |
|---|---|
| Density (g/cm³) | 8.0 - 8.5 |
| Melting Point (°C) | 1350 - 1400 |
| Tensile Strength (MPa) | 900 - 1200 |
| Yield Strength (MPa) | 700 - 1000 |
| Elongation (%) | 20 - 30 |
| Thermal Conductivity (W/m·K) | 10 - 15 |
| Corrosion Resistance | Excellent |
Our Company


Hot Tags: gh4049 superalloy bar - high strength nickel alloy rod for aerospace, astm b637, China gh4049 superalloy bar - high strength nickel alloy rod for aerospace, astm b637 suppliers, nickel pipe welding 200, stainless nickel and alloy piping, nickel tubing 200, nickel alloy 201 tubing, nickel 201 piping, 200 stainless nickel and alloy piping