Inconel 718 Forgings
Forging Types: Forged shafts, forged rings, forged bars, forged discs, forged billets, forged blocks, forged flanges
Specifications & Cutting Service: Custom dimensions available, precision cutting service supported
Applicable Standards: ASTM B637, AMS 5662, AMS 5663
Core Properties: High tensile strength, good low-temperature toughness, age-hardenable
Testing & Certification: UT, PT NDT inspection, 3.1 / 3.2 material test certificates provided
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Which standard covers Inconel 718 forgings?
Forgings in Inconel 718 (UNS N07718) are ordered to the forging-specific ASTM/ASME specification shown in the standards table above - commonly ASTM B564 / ASME SB-564 for corrosion-resistant alloys and ASTM B637 / ASME SB-637 for age-hardened high-temperature alloys - not to the bar, plate or tube standard. State the UNS designation, forging class, drawing, test orientation and delivery condition on the purchase order.

Inconel 718 Forgings - Specification Overview
Inconel 718 forging is a Gamma-double-prime precipitation-hardened Ni-Fe-Cr hot-worked product manufactured to the forging-specific ASTM/ASME specification listed in the standards table below. With UNS designation N07718, the material is produced by VIM + ESR/VAR melting, cogging and upsetting, open- or closed-die forging or ring rolling with controlled grain flow, followed by heat treatment and machining. Forging form changes the acceptance logic relative to bar: grain flow, transverse / tangential tensile properties, macrostructure, grain size and 100% volumetric ultrasonic soundness become the controlling tests. Every forging is delivered with an EN 10204 3.1 mill test certificate recording heat number, actual chemistry, mechanical results in the specified orientation and the full forging heat-treatment record.
Inconel 718 Forgings International Grade Equivalents
Cross-reference is for identification only. Equivalent grades are nominally similar, not automatically interchangeable: chemical limits, impurity control, heat treatment and acceptance testing differ between national standards. Always confirm by UNS number and product-form standard.
| Designation system | Equivalent grade |
|---|---|
| DIN W.Nr. | 2.4668 |
| EN | NiCr19Fe19Nb5Mo3 |
| GB | GH4169 |
| JIS | NCF 718 |
Inconel 718 Forgings Applicable Standards for Forgings
ASTM/ASME specifications are product-form specific: the bar, plate, tube, strip, forging and filler-metal standards for the same UNS designation carry different test and acceptance requirements. State the governing product-form standard and edition on the purchase order.
| Region / system | Specification |
|---|---|
| Grade-specific governing standard | ASTM B637 / ASME SB-637 (bar and forgings) |
| United States (forgings) | ASTM B564 / ASME SB-564 for corrosion-resistant nickel alloy forgings; ASTM B637 / ASME SB-637 for precipitation-hardening and high-temperature alloy forgings |
| Related forging specifications | ASTM B462 and ASTM A182 / ASME SA-182 where the alloy and construction code require them |
| Aerospace (AMS) | AMS 5662 / AMS 5666 and the grade-specific AMS forging specification listed in the standards table |
| China | GB/T 14992 (GH series) / GB/T 15007 (NS series) chemistry; forging product standard per the order |
| Europe | EN 10222-5 / EN 10095 basis; EN 10204 3.1 certificate governs the delivered heat |
| Testing standards | ASTM E8 tensile (including transverse / tangential tests), hardness, grain size, macrostructure, ultrasonic examination, PMI |
| Other product forms of this grade | ASME SB-637; ASTM B670 plate; B444 tube; AMS 5596; GB/T 14999; EN 10095 |
Inconel 718 Forgings Chemical Composition (wt%)
Published specification limits for the base alloy, N07718. Single figures are maximum values unless a range or min is shown. The certified heat analysis on the EN 10204 3.1 MTC governs; the Forgings product standard invokes its own check-analysis and acceptance requirements.
| Element / item | Limit (wt%) |
|---|---|
| Ni | 50.0-55.0 |
| Cr | 17.0-21.0 |
| Fe | balance |
| Nb+Ta | 4.75-5.50 |
| Mo | 2.8-3.3 |
| Ti | 0.65-1.15 |
| Al | 0.20-0.80 |
| Co | 1.0 max |
| C | 0.08 max |
| Mn | 0.35 max |
| Si | 0.35 max |
| B | 0.006 max |
Data basis: the published ASTM / ASME / AMS / EN / DIN / GB / JIS documents listed above and recognised producer data sheets. Refer to the current edition of the governing standard for the complete table including residual and impurity elements.

Inconel 718 Forgings Mechanical and Physical Properties
Values quoted are published specification minima or typical solution-annealed data for the base alloy. The delivered forging is accepted to its own product-form standard; properties vary with section size, cold work, test orientation and temperature, and the certified results on the MTC govern.
| Property | Value |
|---|---|
| Tensile strength, Rm | 1240 MPa min (aged) |
| Yield strength, Rp0.2 | 1035 MPa min (aged) |
| Elongation, A | 10% min |
| Density | 8.19 g/cm3 |
| Melting range | 1260-1336 C |
| Temperature capability | 650 C (gamma-double-prime solvus ~680 C) |
Inconel 718 Forgings Sizes, Tolerances and Supply Condition
The following capabilities apply specifically to the forging form of Inconel 718; other product forms are covered by their own standards and dimensional schedules. Values reproduce the capability already published on the Forgings hub page and are confirmed against the drawing or order specification before release.
| Parameter | Forgings capability |
|---|---|
| Forging types | Open-die and closed-die forgings, rolled rings, discs, hubs, flanges, blocks, shafts and step shafts, upset forgings |
| Ring / disc capability | OD up to 2,500 mm; height up to 600 mm |
| Forged bar | Diameter up to 800 mm; longer step shafts by agreement |
| Weight range | From small precision forgings to multi-tonne open-die pieces; quoted per drawing |
| Manufacturing route | VIM + ESR/VAR melting → cogging / upsetting → open or closed die forging or ring rolling with controlled grain flow → heat treatment → rough / finish machining |
| Dimensional tolerance | Per drawing and the governing forging specification; machining allowance stated on the forging drawing |
| Delivery condition | Solution annealed, annealed, aged / precipitation-hardened, or as-forged; rough-machined or finish-machined on request |
| Inspection | Chemical analysis, ASTM E8 tensile in the required orientation, hardness, grain size, macro / microstructure, 100% ultrasonic examination, liquid penetrant where specified, dimensional check, PMI |
| Documentation | EN 10204 3.1 MTC (3.2 on request), forging heat-treatment chart with furnace records, UT report, NACE MR0175 / ISO 15156 statement when specified |
Inconel 718 Forgings Heat Treatment
Inconel 718 is a precipitation-hardened nickel-based superalloy. Forgings rely on precise solution annealing combined with a two-stage aging treatment to precipitate strengthening γ″ and γ′ phases, achieving high strength, creep resistance, and fatigue resistance to meet the demands of rotating aerospace components.
The full STA (solution treated and aged) cycle under AMS 5663 consists of solution treatment at 955–980°C, holding at 720°C for 8 hours, furnace cooling to 620°C with an 8-hour hold, followed by air cooling. AMS 5662 performs solution treatment only, leaving the material relatively soft and suitable for customers who wish to age-harden components after machining. A stress-relief step can be added after heavy rough machining. Furnace temperature charts are recorded for all heat treatments, followed by hardness and PMI re-inspections after heat treatment.
| Heat Treatment Condition | Temperature & Cycle | Cooling | Application Notes |
|---|---|---|---|
| AMS 5663 (Solution + Double Aging, STA) | Solution 955–980 °C; 720 °C × 8 h → furnace cool to 620 °C × 8 h | Air cool final step | Final high-strength condition for turbine disks, fastener forgings |
| AMS 5662 (Solution Only) | Solution 955–980 °C | Air cool | Soft machinable state, customer performs aging after machining |
| Stress Relief (Optional) | 650–760 °C, hold 2–4 h | Slow air cool | For heavily machined forgings to lower machining residual stress |
Characteristics of Inconel 718 forging
Gamma-double-prime (Ni3Nb) gives the highest yield strength of any widely used wrought superalloy bar
slow gamma-prime response allows welding without strain-age cracking
retains strength from cryogenic to 650 C
readily forged into large-diameter billet
In forged form these characteristics translate into component integrity: the Gamma-double-prime precipitation-hardened Ni-Fe-Cr chemistry sets hot-workability, forge-temperature window and response to solution annealing or ageing, while the forging reduction and grain-flow pattern govern anisotropic strength and fatigue life. Test pieces are taken in the orientation required by the governing forging specification, and the whole volume is ultrasonically examined before machining.
Inconel 718 Forgings Applications
- Gas-turbine discs and shafts
- high-strength fasteners and studs
- rocket-engine turbopump shafts
- downhole drilling tools
- nuclear core components
- die and tooling blocks
- Rotating discs, hubs, shafts and compressor / turbine hardware
- Pressure-containing flanges, rings and valve bodies to ASME SB-564 / SB-637
- Large rings and upset forgings for aerospace and power-generation assemblies
Typical service envelope: 650 C (gamma-double-prime solvus ~680 C). Final material selection should be confirmed against the actual medium, concentration, pressure, stress level and applicable design code.

Packaging and Shipping

This photo shows finished Inconel 718 nickel alloy forgings in warehouse, ready for shipment, including forged blocks, forged rings and forged sleeves. All parts are solution treated and age hardened, passed UT and PT non-destructive testing. Bubble wrap is used for surface protection, fixed on solid wooden pallets to prevent scratches and impact damage during transit. We supply to ASTM B637, AMS 5662 specifications, custom sizes available with full material traceability certificates.
Nickel-Alloy Forgings: Inconel 600/601/625, Monel 400/K500, Hastelloy C276/C22, Incoloy 800/800H/800HT→ASTM B564
FAQ:
Which standard covers Inconel 718 forgings?
Forgings in Inconel 718 (UNS N07718) are ordered to the forging-specific ASTM/ASME specification shown in the standards table above - commonly ASTM B564 / ASME SB-564 for corrosion-resistant alloys and ASTM B637 / ASME SB-637 for age-hardened high-temperature alloys - not to the bar, plate or tube standard. State the UNS designation, forging class, drawing, test orientation and delivery condition on the purchase order.
What forging sizes and shapes can GNEE supply in Inconel 718?
Open-die and closed-die forgings, rolled rings, discs, hubs, flanges, blocks and step shafts; rings / discs up to 2,500 mm OD and 600 mm height, forged bar up to 800 mm diameter. Rough or finish machining, controlled grain flow and customer-specific forging drawings are supported.
How is a Inconel 718 forging inspected and certified?
Each forging receives chemical analysis, ASTM E8 tensile testing in the orientation required by the specification, hardness, grain-size and macrostructure examination, 100% ultrasonic examination, liquid penetrant when specified, dimensional checking and PMI. The EN 10204 3.1 MTC is accompanied by the forging heat-treatment chart, UT report and, when required, EN 10204 3.2 third-party endorsement.
What is the chemical composition of Inconel 718 forging?
The governing limits are: Ni 50.0-55.0; Cr 17.0-21.0; Fe balance; Nb+Ta 4.75-5.50; Mo 2.8-3.3; Ti 0.65-1.15. The full table on this page is taken from the published specification for the base alloy and is verified on the EN 10204 3.1 certificate. Composition is the controlling identifier; a trade name alone is not a complete purchase specification. Published specification limits for the base alloy, N07718. Single figures are maximum values unless a range or min is shown. The certified heat analysis on the EN 10204 3.1 MTC governs; the Forgings product standard invokes its own check-analysis and acceptance requirements.
What heat treatment applies to Inconel 718 forging?
Solution treat 955-980 C then age 720 C / 8 h, furnace cool to 620 C / 8 h, air cool (AMS 5663 condition). Hangbo records the actual furnace cycle on the certificate; any re-heat-treatment after machining or forming must follow the same qualified cycle and the governing product standard.
What mechanical properties does Inconel 718 achieve in forging form?
Base-metal specification values for the quoted condition are: tensile 1240 MPa min (aged), yield 1035 MPa min (aged), elongation 10% min. These are the values published for the base alloy; the delivered forging is accepted to its own product standard, and the certified test results on the MTC govern rather than a data sheet assumption.
Where is Inconel 718 forging typically used?
Gas-turbine discs and shafts; high-strength fasteners and studs; rocket-engine turbopump shafts. Final selection should be confirmed against the actual medium, temperature, stress level and applicable design code; our engineers can review the service condition before quotation.
Hot Tags: inconel 718 forgings, China inconel 718 forgings suppliers
Previous
No InformationYou Might Also Like
Send Inquiry