Why Alloy 718 Is Classed as a Superalloy

What Makes an Alloy a Superalloy

A superalloy is a metal designed to operate at a high fraction of its melting temperature while retaining strength and surface stability. Three families exist: nickel base, cobalt base and iron-nickel base. The defining requirements are mechanical strength and creep resistance at elevated temperature, resistance to oxidation and hot corrosion, and sufficient damage tolerance and fatigue resistance for cyclic service.

Alloy 718 (UNS N07718) meets all three. It retains useful strength to about 700 C, resists oxidation through a chromium rich surface oxide, and combines that with the toughness and weldability needed for large structures. A conventional austenitic stainless steel loses a large part of its strength well below that temperature, and a carbon or low alloy steel loses most of it, which is precisely why the superalloy category exists.

The Metallurgy Behind the Classification

The strength of 718 comes from precipitation hardening. Solution annealing at approximately 980 C dissolves the alloying elements into a single phase matrix. Subsequent ageing precipitates a fine dispersion of the gamma-double-prime phase, Ni3Nb, which is coherent with the matrix and strongly impedes dislocation motion. A secondary gamma-prime precipitate contributes as well, and the combination produces the strength level that defines the grade.

Element Typical Range (wt%) Metallurgical Role
Nickel (Ni) 50.0 - 55.0 Face centred cubic matrix; provides toughness and phase stability.
Chromium (Cr) 17.0 - 21.0 Forms the protective oxide that resists oxidation and hot corrosion.
Niobium + Tantalum (Nb+Ta) 4.75 - 5.50 Principal gamma-double-prime former; slow ageing kinetics improve weldability.
Molybdenum (Mo) 2.80 - 3.30 Solid solution strengthening and improved corrosion resistance.
Titanium (Ti) 0.65 - 1.15 Gamma-prime former; controls the ageing response.
Aluminium (Al) 0.20 - 0.80 Gamma-prime former; balanced against titanium.

Niobium is the element that distinguishes 718 from earlier precipitation hardening grades. Because gamma-double-prime precipitates slowly, the alloy can be welded and then aged without the strain age cracking that limits the weldability of some gamma-prime strengthened nickel alloys.

Properties That Justify the Superalloy Label

In the correctly aged condition, 718 typically delivers yield strength in the region of 1030-1150 MPa and tensile strength in the region of 1240-1400 MPa at room temperature, with hardness in the range of about 36-42 HRC. Those values are maintained at elevated temperature far better than in steel, and the alloy also performs well at cryogenic temperatures, retaining toughness where many materials become brittle.

Oxidation resistance comes from the chromium content: a thin, adherent chromium rich oxide forms on heating and limits further attack. Creep resistance comes from the stability of the precipitate structure, which resists coarsening far better than the carbides that carry strength in lower alloyed steels.

Acceptance of these properties is tied to the material specification. AMS 5662 and AMS 5663 are the usual aerospace documents for 718 bar, forgings and forging stock, with tension testing to ASTM E8/E8M, hardness testing to ASTM E18 and grain size determination to ASTM E112. AGH4169 and GH4169 are the equivalent Chinese designations for the same chemistry.

Where the Premium Is Justified

Superalloy pricing is only defensible where the operating envelope cannot be met by a cheaper material. Typical 718 applications include gas turbine discs, compressor and turbine shafts, casings, combustion hardware supports, aerospace fasteners, cryogenic tankage and piping, and oil and gas downhole components such as valve stems and high pressure wellhead parts.

The common thread is a requirement that survives the substitution test: if a lower cost stainless steel could be used within the same size envelope and service life, the specification would already have moved there. When it has not, the driving factors are usually elevated temperature strength, fatigue life under cyclic loading, or the need to avoid a strength reduction caused by welding.

Fabrication Considerations

Alloy 718 machines in the annealed condition and is usually finished after ageing, using sharp positive rake tooling, rigid setups and high pressure coolant because of the alloy's high shear strength, work hardening tendency and low thermal conductivity. Welding is performed by gas tungsten arc, gas metal arc, electron beam or resistance methods with matching filler metal, and the work area must be free of sulphur and lead bearing contaminants such as certain marking crayons and lubricants, which cause heat affected zone cracking.

Heat treatment must be qualified rather than assumed. The standard two-step age, approximately 8 hours at 720 C followed by a controlled cool and 8 hours at about 620 C, is what produces the specified properties, and any deviation changes the delivered strength even if the chemistry is unchanged.

Frequently Asked Questions

Q: Why is Alloy 718 called a superalloy?
A: Because it retains high strength, creep resistance and oxidation resistance at a high fraction of its melting range, roughly up to 700 C, which conventional steels cannot do.

Q: What is the UNS number for Alloy 718?
A: UNS N07718. The Chinese equivalent designations AGH4169 and GH4169 refer to the same chemistry.

Q: What strengthens Alloy 718?
A: A coherent gamma-double-prime precipitate, Ni3Nb, formed during a two-step ageing treatment after solution annealing, with some contribution from gamma-prime.

Q: Is Alloy 718 weldable?
A: Yes, it is one of the more weldable precipitation hardening superalloys, because the slow precipitation kinetics of gamma-double-prime reduce the risk of strain age cracking.

Q: What is the maximum service temperature of Alloy 718?
A: Approximately 700 C for long term service, above which creep and oxidation become the limiting factors and a higher chromium or higher refractory grade is normally considered.

Q: Which specifications cover Alloy 718 bar and forgings?
A: AMS 5662 and AMS 5663 for aerospace quality bar, forgings and forging stock, supported by tension testing to ASTM E8/E8M and hardness testing to ASTM E18.