1. Pure Nickel vs. Carbon Steel
Tensile strength: ~345 MPa (megapascals) in its annealed state.
Yield strength: ~140 MPa.
It is ductile and malleable, making it unsuitable for high-strength applications in its pure form.
Tensile strength: ~400–550 MPa.
Yield strength: ~250–350 MPa.
Thus, pure nickel is weaker than most carbon steels.
2. Nickel Alloys vs. High-Strength Steels
Inconel 718: Tensile strength ~1,300 MPa (after heat treatment); retains strength even at 650–700°C.
Hastelloy C-276: Tensile strength ~895 MPa, with exceptional corrosion resistance.
Maraging steel (18Ni): A low-carbon, high-nickel steel with tensile strength up to 2,400 MPa, achieved through precipitation hardening.
High-strength low-alloy (HSLA) steel: Tensile strength up to 800 MPa, with good toughness.
Tool steels: Tensile strength ranging from 1,500–2,000 MPa, depending on heat treatment.
3. High-Temperature Performance
Inconel 718 retains ~60% of its room-temperature strength at 700°C.
Even heat-resistant steels (e.g., stainless steel 310) lose significant strength above 800°C, making nickel alloys stronger in high-heat environments like gas turbines or jet engines.




4. Hardness
Pure nickel has a Brinell hardness of ~60 HB.
Mild steel has a Brinell hardness of ~120–150 HB.
High-strength steels (e.g., hardened tool steel) can reach 60 HRC (Rockwell C), equivalent to ~700 HB-far harder than nickel alloys (typically 20–40 HRC).
At room temperature: Most steels (especially high-strength or alloy steels) are stronger than pure nickel and even many nickel alloys.
At high temperatures: Nickel-based superalloys surpass nearly all steels in strength retention.
Steel, in its advanced forms, is generally stronger than nickel, but nickel alloys dominate in high-temperature and corrosive environments where strength must be maintained under extreme conditions.