Alloy 718 and alloy X-750 are both age-hardenable nickel alloys used in gas turbine, nuclear and spring applications, and they are often specified on the same drawing. They differ in base chemistry, in the type of precipitate that forms, and in how tolerant they are to welding.
Family and Strengthening Route
Alloy 718 (UNS N07718) is a nickel-iron-chromium alloy in which the iron content is the balance of the composition, typically around 18 percent. It is hardened by a controlled solution treatment followed by a two-step aging treatment that precipitates gamma-double-prime and gamma-prime phases. Alloy X-750 (UNS N07750) is a nickel-chromium-iron alloy with a minimum nickel content of 70 percent, and it hardens through gamma-prime formation driven mainly by titanium and aluminium. Both are supplied in a solution-treated condition for forming and then aged after fabrication, or supplied already aged when the part geometry is final.
Chemistry Compared
| Element | Alloy 718 (N07718) | Alloy X-750 (N07750) |
|---|---|---|
| Nickel | 50.0-55.0 | 70.0 min |
| Chromium | 17.0-21.0 | 14.0-17.0 |
| Iron | Balance | 5.0-9.0 |
| Niobium + tantalum | 4.75-5.50 | 0.70-1.20 |
| Titanium | 0.65-1.15 | 2.25-2.75 |
| Aluminium | 0.20-0.80 | 0.40-1.00 |
| Molybdenum | 2.80-3.30 | - |
The practical consequences follow directly from this table. Alloy 718 contains molybdenum, which X-750 does not, and that lifts its resistance to reducing corrosion. Alloy 718 also carries a higher chromium level, so it oxidises more slowly at temperature. Alloy X-750, in contrast, contains almost three times the titanium of 718, which is what makes it so responsive to aging and so attractive for springs and fasteners.
Mechanical Properties
Alloy 718 in the precipitation-hardened condition is specified to a minimum tensile strength of 1241 MPa (180 ksi), a minimum 0.2 percent yield strength of 1034 MPa (150 ksi) and a minimum elongation of 12 percent. Alloy X-750 in the aged condition offers a lower yield strength than 718 but retains useful strength to higher temperatures and shows excellent relaxation resistance, which is why it dominates spring and bolting applications up to roughly 650 °C. Density also differs: 718 is about 8.19 g/cm3 and X-750 is about 8.28 g/cm3.
Welding and Fabrication
Alloy 718 has good weldability in both the solution-treated and aged conditions and a high resistance to strain-age cracking, so it is standard for large welded fabrications in aerospace and energy hardware. Alloy X-750 is more sensitive to strain-age cracking during post-weld aging, and procedures for it are correspondingly more restrictive, with careful control of restraint, preheat practice and aging cycle. Neither alloy is intended for aggressive chloride or reducing-acid service; for those duties a molybdenum-bearing solid-solution alloy is selected instead.
Standards and Product Forms
Bars, forgings and forging stock: ASTM B637 covers precipitation-hardening nickel alloys including UNS N07718.
Plate, sheet and strip for 718: ASTM B670.
Aerospace material specifications: AMS 5662, AMS 5663 and AMS 5664 cover 718 bar, forging and ring stock in solution-treated and aged conditions, and AMS 5832 covers 718 welding wire.
Threaded fasteners and springs are frequently ordered to drawings that invoke the same ASTM or AMS compositions with additional dimensional and inspection requirements.
Selection Guidance
Specify 718 when the part needs the highest available yield strength, when it will be welded and then aged, or when it must resist mildly reducing environments in addition to heat. Specify X-750 when the duty is spring, seal or fastener work with sustained load at temperature, when relaxation resistance matters more than peak strength, and when the hardware can be aged under properly controlled conditions.
Frequently Asked Questions
Q: Is alloy X-750 stronger than alloy 718?
A: No. In the aged condition 718 develops a higher yield strength, with a specified minimum of 1034 MPa (150 ksi). X-750 is valued for retention of load at elevated temperature and for spring performance rather than for peak room-temperature strength.
Q: Why is alloy 718 easier to weld than X-750?
A: Alloy 718 has a high resistance to strain-age cracking, so it tolerates the restraint and thermal cycles of welding before aging. X-750 is more prone to that cracking mechanism and requires tighter welding and aging procedures.
Q: Does alloy 718 contain molybdenum?
A: Yes, 2.80-3.30 percent. Alloy X-750 contains no deliberate molybdenum addition, which is why 718 resists reducing corrosion better while X-750 relies on its high nickel content for chemical stability.
Q: Which alloy is used for springs and fasteners?
A: X-750 is widely used for springs, seals and high-temperature fasteners because it retains load and resists relaxation at temperature. Alloy 718 is used for high-strength structural and rotating components that also need weldability.
Q: How should the two alloys be ordered?
A: Specify UNS N07718 with ASTM B637 or B670 for 718 bar and flat product, and UNS N07750 with the applicable ASTM or AMS material specification for X-750. Always state the heat treatment condition so that the supplier can certify the correct mechanical properties.