Stainless steel is not one material but a family of iron-based alloys in which chromium is the defining addition. The internationally accepted threshold is a minimum chromium content of 10.5 percent, and it is that chromium level which allows a stable, self-renewing oxide film to form on the surface.
What Makes a Steel "Stainless"
Carbon content across the family runs from roughly 0.03 percent in the low-carbon grades up to about 1.2 percent in some martensitic and tool grades. Chromium governs corrosion resistance; nickel, molybdenum, nitrogen, titanium and niobium are added to control structure, strength and resistance to particular forms of attack. Where oxygen is available the chromium-rich passive layer re-forms within seconds of being scratched, cut or machined, which is why the surface keeps a clean appearance under normal working conditions.
Five metallurgical families cover almost all commercial supply: austenitic, ferritic, martensitic, duplex (austenitic-ferritic) and precipitation-hardening. Austenitic grades account for the largest share of tonnage because they combine formability, weldability and toughness from cryogenic temperatures to roughly 550 °C in continuous service.
Typical Grades and Chemistry
| Grade | UNS | EN | Cr (%) | Ni (%) | Mo (%) | PREN |
|---|---|---|---|---|---|---|
| 304 | S30400 | 1.4301 | 18.0-20.0 | 8.0-10.5 | - | ~18 |
| 304L | S30403 | 1.4307 | 18.0-20.0 | 8.0-12.0 | - | ~18 |
| 316L | S31603 | 1.4404 | 16.0-18.0 | 10.0-14.0 | 2.00-2.50 | 24-26 |
| 2205 duplex | S32205 | 1.4462 | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 34-36 |
The pitting resistance equivalent number is calculated as Cr + 3.3 Mo + 16 N and is a quick screening index for chloride service. The 0.03 percent carbon ceiling on the "L" grades is what prevents sensitisation, the chromium carbide precipitation that otherwise leaves grain boundaries vulnerable after welding.
Product Forms and Governing Standards
Flat products - plate, sheet and strip: ASTM A240/A240M, with EN 10088-2 for European supply; dimensional tolerances and finishes are covered by ASTM A480/A480M.
Long products - bars, wire rod and profiles: ASTM A276/A276M, or EN 10088-3.
Seamless and welded pipe: ASTM A312/A312M, supported by ASTM A1016/A1016M for general tube requirements.
Welded mechanical tubing: ASTM A554.
Corrosion Behaviour and Selection Limits
The passive film performs well in oxidising environments but is vulnerable in two familiar ways. Chlorides break the film down locally and cause pitting and crevice attack, so 304 is usually restricted to mildly chloride-bearing water while 316L and duplex 2205 extend the chloride tolerance considerably. Austenitic grades can also suffer chloride stress corrosion cracking once metal temperatures rise above roughly 60 °C in the presence of chlorides, and that is exactly the regime where duplex or higher-alloyed grades are selected. In strongly reducing acids, molybdenum content rather than chromium alone decides how the alloy performs.
Fabrication and Supply Notes
Cold working raises the strength of austenitic grades but also makes them slightly magnetic, so magnetic response is not a dependable identification test. After welding, welds and heat-affected zones should be cleaned and passivated in line with ASTM A380 so that the chromium oxide layer is restored uniformly. A purchasing specification should always state grade, product form, the applicable ASTM or EN specification, surface finish and any corrosion or impact test requirement, because those five items determine the processing route and the final price per tonne.
Frequently Asked Questions
Q: Is stainless steel magnetic?
A: The austenitic grades 304 and 316 are essentially non-magnetic in the annealed condition. Cold working, such as drawing or bending, can make them mildly magnetic, and ferritic and martensitic grades are magnetic from the outset, so a magnet cannot be used to verify a grade.
Q: What is the difference between 304 and 316?
A: 316 contains 2.00-2.50 percent molybdenum while 304 contains none. That molybdenum lifts the pitting resistance equivalent number from about 18 to 24-26, giving 316 and 316L far better resistance to chlorides and to reducing acids.
Q: What does the "L" suffix stand for?
A: It denotes a low-carbon variant with a maximum of 0.030 percent carbon, as in 304L and 316L. The lower carbon level prevents chromium carbide precipitation in the heat-affected zone of welds, so heavy sections can be welded without a post-weld solution anneal.
Q: Can stainless steel still rust?
A: Yes. If the passive film is destroyed by chlorides, reducing acids, embedded iron contamination or lack of oxygen in a crevice, localised corrosion can start. Correct grade selection, good drainage, clean fabrication and passivation are what keep the alloy rust-free.
Q: Which surface finishes are commonly supplied?
A: Cold-rolled 2B, bright annealed, satin or brushed No. 4, and hot-rolled No. 1 for plate are the standard mill finishes. Finishes are defined in ASTM A480/A480M, and a rougher finish generally gives slightly better pitting resistance in chloride service.
Q: Which standard should be quoted on a purchase order?
A: Quote the product form first, then the specification: ASTM A240 for plate, sheet and strip, ASTM A276 for bar, ASTM A312 for pipe, or the equivalent EN 10088 part. Adding the grade, UNS number and any extra test requirement removes any ambiguity for the mill.