Why This Alloy Is Selected for Exhaust Systems
Inconel 625 is a nickel-chromium-molybdenum alloy with niobium plus tantalum additions that give it a combination of high temperature strength, oxidation resistance and fatigue resistance in one material. In an exhaust system the tube sees a mixed duty: hot gas on the inside, cooling air and thermal cycling on the outside, and vibration from the engine or structure. Stainless steel handles that duty until the metal temperature climbs high enough for scaling and for a drop in fatigue strength, at which point a nickel based tubing becomes the practical option.
The alloy keeps useful strength to roughly 980 degrees Celsius in oxidising service and is tough at cryogenic temperature as well, which is why the same tubing is used in both hot exhaust runs and cold sections of the same system. The niobium addition raises the creep strength of the solid solution matrix without the need for a precipitation heat treatment, so a welded structure does not require a post-weld ageing treatment.
Tube Specifications and Standard Dimensions
| Standard | Product | Notes |
|---|---|---|
| ASTM B444 | Seamless pipe and tube of UNS N06625 | Grade 1 annealed and Grade 2 solution annealed conditions |
| ASTM B704 | Welded tube of UNS N06625 | Cold worked and annealed as ordered |
| ASTM B705 | Welded pipe of UNS N06625 | Larger nominal sizes for headers |
| ASTM B751 | General requirements | Permissible variations, testing and inspection provisions |
| ASME SB444 | Code equivalent of B444 | Used where the piping is code stamped |
Exhaust tubing is generally ordered to outside diameter and wall thickness rather than to nominal pipe size, because it is bent and formed. Common forms run from small diameter lines for sensor and bleed pipes up to larger ducts for main exhaust runs, with bellows sections made from very thin wall tube to absorb thermal expansion. Because thin walls offer little corrosion allowance, both surfaces are normally supplied clean and free of embedded iron, and the tube is delivered in the annealed condition to retain ductility for bending.
Mechanical Requirements and Temperature Behaviour
| Property at room temperature | Grade 1, annealed | Grade 2, solution annealed |
|---|---|---|
| Tensile strength, minimum | 827 MPa | 758 MPa |
| Yield strength, minimum | 414 MPa | 379 MPa |
| Elongation, minimum | 30 percent | 30 percent |
Both conditions are covered by ASTM B444 for seamless tube, and the purchaser must state which is required, because the two have different minimum strengths and different heat treatment histories. Grade 1 is annealed at a lower temperature and retains higher strength; Grade 2 is solution annealed at a higher temperature, which gives better resistance to intergranular attack and better ductility for severe forming. For exhaust service, the choice is normally driven by the forming operation and by the maximum metal temperature rather than by strength alone.
Fabrication: Bending, Welding and Stress Relief
The alloy work hardens quickly, so bending schedules call for generous bend radii and for intermediate annealing where a tight radius is unavoidable. Welding is done with a matching nickel-chromium-molybdenum filler classified ERNiCrMo-3 under AWS A5.14, with argon shielding and a purged root, and with the same contamination precautions that apply to any nickel alloy: sulphur, lead, copper and zinc must be kept away from the joint. Heat input is controlled to limit distortion, and interpass temperature is normally held under about 150 degrees Celsius. Solution annealing, where required after cold forming, is carried out at high temperature followed by rapid cooling, and the temperature must be specified on the process sheet because it controls both corrosion resistance and strength.
Inspection and Quality Requirements
Seamless and welded exhaust tube is normally examined by an electromagnetic eddy current test to ASTM E571, with hydrostatic or pneumatic pressure testing as specified on the order. Dimensions, wall thickness and straightness are checked under ASTM B751, which also sets the permissible variations for these products. Where the tubing forms part of a code stamped system, the material must be ordered to the ASME equivalent specification and supplied with a certified test report, and the weld procedure and welders must be qualified to the applicable section of the code. Extra testing such as intergranular corrosion evaluation or a flattening test is added for thin walls intended to be expanded or bent.
Frequently Asked Questions
Q: What specification covers Inconel 625 exhaust tubing?
A: Seamless tube is ordered to ASTM B444, welded tube to ASTM B704, and welded pipe to ASTM B705, all with the general requirements of ASTM B751.
Q: Should I use Grade 1 or Grade 2 for exhaust tube?
A: Grade 1 annealed gives higher minimum strength at 827 MPa tensile, while Grade 2 solution annealed gives better ductility and intergranular corrosion resistance. The choice follows the forming operation and the maximum metal temperature.
Q: What filler is used for welding this tubing?
A: A matching nickel-chromium-molybdenum filler classified ERNiCrMo-3 under AWS A5.14, welded with argon shielding and a purged root.
Q: Up to what temperature can the tubing be used?
A: Roughly 980 degrees Celsius in oxidising service, with the exact limit set by the stress, the cycle frequency and the atmosphere. Reducing or sulphur-bearing gases lower the usable temperature.
Q: Why is thin wall bellows tubing so sensitive to contamination?
A: There is almost no wall thickness to absorb corrosion, and sulphur or low melting point metals picked up from tooling cause rapid cracking in a thin section under vibration.
Q: What non-destructive test is normally applied?
A: An electromagnetic eddy current examination to ASTM E571, supplemented by hydrostatic or pneumatic testing when the order specifies it.