Nov 11, 2025 Leave a message

What are the characteristics of CUZN30

1.What are the characteristics of CUZN30?

Chemical Composition: Primarily 69–71% Cu and 29–31% Zn, with trace impurities (e.g., lead ≤0.07%, iron ≤0.05%) to optimize performance.

Microstructure: Alpha-beta (α+β) phase structure, combining the ductility of alpha brass and the strength of beta brass.

Machinability: Excellent – rated as one of the most machinable brass alloys (machinability index ≈85%, compared to 100% for free-cutting steel). It produces clean chips and requires minimal tool wear.

Formability: Good cold and hot workability; can be forged, extruded, bent, and stamped, though less ductile than alpha brasses (e.g., CUZN15).

Corrosion Resistance: Moderate – resistant to atmospheric corrosion, fresh water, and neutral salts, but susceptible to dezincification in aggressive environments (e.g., hot saline water, acidic solutions).

Thermal & Electrical Conductivity: Moderate – thermal conductivity ≈110 W/m·K, electrical conductivity ≈28% IACS (lower than pure copper but sufficient for non-critical electrical applications).

Aesthetic & Other Traits: Golden-yellow appearance; good solderability and brazability; non-magnetic; cost-effective due to balanced material and processing costs.


2.What is the yield strength of CUZN30?

Yield strength varies by heat treatment and processing state (annealed, cold-worked, etc.). Typical values are:

Annealed state (soft, 600–650°C for 1–2 hours, furnace-cooled): Yield strength (Rp0.2) ≈ 170–200 MPa.

Cold-worked state (e.g., 50% cold reduction): Yield strength (Rp0.2) ≈ 400–450 MPa.

Hot-worked state (forged or extruded): Yield strength (Rp0.2) ≈ 220–280 MPa.

Note: Yield strength is measured per ASTM B16/B16M or EN 12164 standards, using a 0.2% offset method.

info-448-449info-445-441

info-445-441info-440-444

3. What is the tensile strength of CUZN30?

Like yield strength, tensile strength depends on processing and heat treatment. Typical values include:

Annealed state: Tensile strength (Rm) ≈ 380–420 MPa.

Cold-worked state (50% cold reduction): Tensile strength (Rm) ≈ 600–650 MPa.

Hot-worked state: Tensile strength (Rm) ≈ 450–500 MPa.

Additional mechanical data for reference: Elongation at break (A50) is 30–40% in the annealed state and 5–10% in the fully cold-worked state.

Summary

CUZN30 is valued for its excellent machinability, balanced strength and formability, and cost-effectiveness. Its yield strength ranges from ~170–450 MPa, and tensile strength from ~380–650 MPa, depending on processing. It is commonly used for turned parts, fasteners, valves, fittings, and mechanical components requiring both precision machining and moderate structural performance.