1) Welding Performance
Inconel 600 is readily weldable using conventional fusion and solid‑state processes.
Common processes: GTAW (TIG), GMAW (MIG), SMAW, SAW, EBW, resistance welding.
Preheat: Typically not required for most thicknesses and ambient temperatures.
Postweld heat treatment (PWHT): Often not mandatory for corrosion resistance or general service, but may be applied to relieve residual stresses (e.g., after heavy fabrication or for thick sections).
Filler metals: Common choices are ERNiCr‑3 (GTAW/GMAW) and ENiCr‑3 (SMAW).
Key considerations:
Keep heat input moderate to avoid grain growth and potential reduction in ductility/impact toughness.
Cleanliness is critical (remove oil, grease, paint, sulfide‑bearing contaminants) to prevent cracking and porosity.
In some cases, interpass cleaning and back purging (especially for thin‑wall pipe) with argon help maintain weld quality.
2) Forming & Fabrication (Hot/Cold Working)
Hot Working
Recommended temperature range: Approximately 980–1150°C (1800–2100°F).
It has good hot ductility in this range, allowing for forging, rolling, extrusion, and upsetting.
Cooling: Air cooling or faster cooling is typically acceptable; slow cooling may lead to carbide precipitation at grain boundaries, which can affect subsequent properties and corrosion resistance (though 600 is less prone to sensitization than some stainless steels).
Cold Working
Inconel 600 is cold formable, but it work‑hardens rapidly.
Multiple passes may require intermediate annealing to restore ductility.
Annealing: Common practice is solution annealing at 1100–1150°C (2010–2100°F) followed by rapid cooling (water quench or air cool, depending on section size).
3) Machinability
Machinability is often rated as poor to moderate relative to AISI 304 stainless steel.
Challenges:
High shear strength and toughness lead to high cutting forces.
Low thermal conductivity causes heat to concentrate at the cutting edge, accelerating tool wear.
Strong work‑hardening means that tool rubbing (e.g., from dull tools or light cuts) can quickly harden the surface, making subsequent passes more difficult.
info-352-347info-348-351
info-348-351info-346-345
Recommended practices:
Use positive‑rake, sharp cutting tools and maintain high cutting speeds with sufficient feed to minimize rubbing.
Apply adequate coolant/lubricant (or use high‑pressure coolant) to reduce heat and chip adhesion.
Use heavy enough depths of cut to engage the unworked material and avoid finishing on a work‑hardened surface layer.
Tool materials: carbides (preferably with wear‑resistant coatings), CBN for finishing (depending on setup), and high‑speed steel (HSS) for lighter operations (though wear will be higher).
Chip control is important; interrupted cuts or appropriate chip‑breaker geometries help manage continuous chips.
4) Heat Treatment
Solution annealing: Primary treatment to homogenize microstructure and restore ductility after cold work.
Stress relief: May be performed at lower temperatures (e.g., 700–900°C / 1290–1650°F) to reduce residual stresses, but this is application‑dependent.
Age hardening: Inconel 600 is not a precipitation‑hardening alloy (unlike Inconel 718), so age hardening to achieve significant strength increases is not typical.
5) Joining to Other Materials
Can be welded to other nickel alloys and stainless steels, but matching filler metals and joint design are important to avoid cracking and ensure corrosion resistance.
Dissimilar metal joints (e.g., to carbon steel) may require consideration of galvanic corrosion and service temperature limitations.