The 2.4669 Nickel Base Superalloy Plate

1. what is the 2.4669 Nickel Base Superalloy Plate?
2.4669 is the EN material designation for a nickel-chromium-molybdenum superalloy, also known as Inconel 625 (trade name) or UNS N06625. It is renowned for exceptional corrosion resistance, high-temperature strength, and weldability.
2.what is the ASTM grade of 2.4669 Nickel Base Superalloy Plate?
The ASTM equivalent grades for 2.4669 include:

ASTM B443/B443M (seamless pipe),

B444/B444M (welded pipe),

B564/B564M (forgings),

B626/B626M (plate, sheet, strip),

B670/B670M (welded tube).

3.What are the mechanical properties of 2.4669 Nickel Base Superalloy Plate?

Tensile Strength: ≥690 MPa (100 ksi)

Yield Strength (0.2% Offset): ≥310 MPa (45 ksi)

Elongation: ≥30%

Hardness: ≤293 HB

Elastic Modulus: ~205 GPa

info-440-442info-445-443

info-444-445info-440-442

4.What is the chemical composition of 2.4669 Nickel Base Superalloy Plate?

Nickel (Ni): ≥58.0% (base element)

Chromium (Cr): 20.0–23.0% (forms protective oxide layer)

Molybdenum (Mo): 8.0–10.0% (enhances resistance to pitting and crevice corrosion)

Niobium + Tantalum (Nb+Ta): 3.15–4.15% (strengthens the alloy via precipitation hardening)

Iron (Fe): ≤5.0%

Carbon (C): ≤0.10%

Silicon (Si): ≤0.50%

Manganese (Mn): ≤0.50%

Phosphorus (P): ≤0.015%

Sulfur (S): ≤0.015%

5.What is the application of 2.4669 Nickel Base Superalloy?

Aerospace: Combustion chambers, turbine blades, exhaust systems.

Marine: Seawater pipelines, offshore platforms, desalination plants.

Chemical Processing: Reactors, heat exchangers, and piping in corrosive environments (e.g., chloride-rich solutions).

Energy: Nuclear power plant components, oil/gas extraction equipment (e.g., sour gas wells).

Environmental: Waste incinerators and flue gas desulfurization systems.