Is INCOLOY a superalloy?

Is INCOLOY a superalloy?

 

Incoloy is used in fluid environments such as sulfuric acid, hydrochloric acid, hydrofluoric acid, phosphoric acid, nitric acid, other acids and freshwater environments.

Incoloy products are primarily chromium- and nickel-based and are designed for corrosion resistance and high-temperature strength.

Incoloy alloy belongs to the super austenitic stainless steel category. One of the advantages of Incoloy alloys is that no heat treatment is required after welding to restore corrosion resistance.


Incoloy 020 "Exhibits excellent corrosion resistance in chemical environments containing sulfuric acid, chloride, phosphoric acid and nitric acid."

Is INCOLOY a superalloy?

Is INCOLOY a superalloy?

Incoloy 028 "Resistant to acids and salts. The copper content makes it resistant to sulfuric acid."

Incoloy 330 "exhibits good strength at elevated temperatures and has good resistance to oxidizing and reducing environments."

Incoloy 800 "remains stable and maintains its austenitic structure even after prolonged exposure to high temperatures."

Incoloy 803 is designed for use in sulfur-rich environments.

Incoloy 825 is approved by ASTM B163 for use in heat exchanger tubes and is approved for pressure vessel operating temperatures up to 525°C or up to 538°C. It "has excellent resistance to sulfuric and phosphoric acid corrosion".

Incoloy 908 "has high tensile strength, resistance to fatigue crack growth, good weldability, metallurgical stability and ductility, high fracture toughness and impact toughness, [and] low coefficient of thermal expansion… [It] resists oxidative embrittlement… …Allows thermal fabrication without cracks."

Incoloy 907 "provides high strength and low coefficient of thermal expansion at temperatures up to 800°F."

Incoloy 945X is designed for use in chlorine-rich environments. Molybdenum enhances the crevice corrosion and pitting resistance of Incoloy 945.

Incoloy MA956 is made through mechanical alloying rather than an integral melting process; it was studied as a space reactor component in the Jimo project. Welding is difficult and requires heating to 200°C during the forming process. A special friction welding process was developed for this purpose.