Apr 01, 2024 Leave a message

Is Nickel Alloy C276 Magnetic? Permeability and Applications

Is Nickel Alloy C276 Magnetic?

Nickel Alloy C276, also designated UNS N10276, is a solution-annealed nickel-molybdenum-chromium alloy with a deliberate tungsten addition. In the standard annealed condition it is essentially non-magnetic at room temperature, and a permanent magnet shows only a negligible pull when it is brought close to the surface.

The reason is microstructural. Alloy C276 is austenitic and keeps a face-centred cubic lattice at room temperature. Ferromagnetism in steels originates from the body-centred cubic ferrite phase, and because C276 contains no ferrite it cannot build up the magnetic domains that make carbon steel and ferritic stainless steel respond strongly to a magnet. Relative permeability values for annealed C276 sit very close to unity, which is why the alloy is treated as a non-magnetic material in instrument building, medical equipment and electrical engineering.

Two practical qualifications matter. First, heavy cold work such as severe bending, swaging or cold drawing can introduce a small magnetic response, because deformation increases dislocation density and can form minor magnetic second phases. Second, an as-welded surface may show a slightly stronger magnetic pull than the parent plate. Both effects are small, and a solution-anneal heat treatment restores the material close to its original non-magnetic state.

Composition of Alloy C276 (UNS N10276)

Element Specified range, wt. %
Nickel (Ni) Balance
Molybdenum (Mo) 15.0 - 17.0
Chromium (Cr) 14.5 - 16.5
Iron (Fe) 4.0 - 7.0
Tungsten (W) 3.0 - 4.5
Cobalt (Co) 2.5 maximum
Manganese (Mn) 1.0 maximum
Silicon (Si) 0.08 maximum
Carbon (C) 0.010 maximum
Phosphorus (P) and Sulfur (S) 0.030 maximum each
Vanadium (V) 0.35 maximum

The very low carbon and silicon limits hold intermetallic precipitation to a minimum during welding, while molybdenum and tungsten together provide the pitting and crevice corrosion resistance that makes the grade suitable for chloride-bearing media.

Magnetic Behaviour Compared with Other Materials

Material Typical magnetic response at room temperature
Carbon steel Strongly magnetic
Martensitic stainless steel (e.g. 410) Magnetic
Austenitic stainless steel 304 or 316 Essentially non-magnetic; slight response after heavy cold work
Nickel Alloy C276 (UNS N10276) Non-magnetic in the annealed condition
Titanium Grade 5 (Ti-6Al-4V) Non-magnetic

A simple workshop check is informative: a strong magnet is attracted firmly to carbon steel, weakly to cold-worked 304 stainless steel, and hardly at all to an annealed C276 part. That test is qualitative only. Where an actual permeability figure is written into a specification, the value should be measured on the specific heat and product form being supplied rather than assumed from the alloy name.

Standards, Product Forms and Corrosion Performance

ASTM B575 / ASME SB575 - plate, sheet and strip of low-carbon nickel-molybdenum-chromium alloy

ASTM B574 / ASME SB574 - rod and bar

ASTM B622 / ASME SB622 - seamless pipe and tube

ASTM B619 / ASME SB619, ASTM B626 / ASME SB626 - welded pipe and tube

ISO 15156 / NACE MR0175 - qualification for oil and gas service containing hydrogen sulfide

C276 is supplied as hot-rolled or cold-rolled plate, bar, seamless and welded tube, sheet and strip, forged and machined components, all in the solution-annealed condition and normally accompanied by an EN 10204 type 3.1 inspection certificate. The combination of high molybdenum and chromium allows the alloy to work in oxidising, reducing and mixed-acid media, and the tungsten addition specifically inhibits pit initiation. Sulfuric acid, hydrochloric acid, phosphoric acid, wet chlorine, hypochlorite solutions and seawater are all routinely handled. C276 also resists chloride-induced stress corrosion cracking, which is the failure mode that limits austenitic stainless steels in hot chloride service.

Typical Industrial Applications

Chemical processing: reactors, columns, heat exchangers and piping exposed to mixed acids

Pollution control: flue gas desulfurisation scrubbers, dampers, stack liners and ducting

Power generation: equipment handling aggressive flue gas condensates

Offshore oil and gas: seawater piping, risers and sour-service components

Pharmaceutical and food processing: vessels, valves and pipework that must be both corrosion resistant and non-magnetic

Because the material is non-toxic and does not become magnetised in service, it is also used for equipment where magnetic interference would disturb instruments or product handling. Non-magnetic behaviour is a property of the annealed product; designers who need a guaranteed permeability limit should state that limit on the purchase order so that the mill can select and verify the correct heat treatment.

Frequently Asked Questions

Q: Is C276 alloy magnetic?
A: No. In the solution-annealed condition nickel alloy C276 is essentially non-magnetic, with relative permeability close to unity.

Q: Why is C276 non-magnetic while carbon steel is strongly magnetic?
A: C276 has a face-centred cubic austenitic structure with no ferrite phase. Ferromagnetism in steel comes from the ferrite phase, so the alloy has no magnetic domains to align.

Q: Can C276 become magnetic after machining or welding?
A: A small magnetic response can appear after heavy cold work or on some as-welded surfaces. Solution annealing normally removes it.

Q: Does its non-magnetic character affect corrosion resistance?
A: No. Magnetic behaviour and corrosion resistance are independent properties, and the corrosion performance of C276 depends on composition and heat treatment rather than on magnetism.

Q: What is the difference between C276 and C22?
A: Both are nickel-molybdenum-chromium alloys, but C22 (UNS N06022) is formulated with a lower iron and tungsten content for improved resistance to oxidising media, while C276 retains its tungsten addition for pitting resistance in reducing acids.

Q: Is C276 suitable for chloride-containing service?
A: Yes. The molybdenum, chromium and tungsten content gives good resistance to pitting and crevice corrosion and to chloride stress corrosion cracking in many industrial environments.