Is alloy C the same as Hastelloy?
Alloy C-276 is an improved forged version of Alloy C, offering the same excellent corrosion resistance as the material but with greatly improved machinability. It can be hot processed and cold formed through conventional procedures.
Mechanical Property Requirements |
|||||
---|---|---|---|---|---|
Ultimate Tensile |
Yield Strength (0.2% OS) |
Elong. in 2 in. (50.8mm) or 4D min,% |
R/A |
Hardness |
|
Min |
100 KSi |
41 KSi |
40 |
||
Max |
|||||
Min (Metric) |
690 MPa |
283 MPa |
|||
Max |
Chemical Requirements |
|||||||
---|---|---|---|---|---|---|---|
Ni |
Cr |
Mn |
Mo |
C |
Si |
Fe |
|
Max % |
Bal. |
16.5 |
1.0 |
17.0 |
0.010 |
0.08 |
7.0 |
Min % |
14.5 |
15.0 |
4.0 |