How does the elastic modulus of Inconel 600 change with temperature

1.How does the elastic modulus of Inconel 600 change with temperature?
The elastic modulus (Young's modulus) of Inconel 600 is strongly temperature-dependent and decreases gradually as temperature increases. This is a typical behavior for nickel-based superalloys. Typical values for the elastic modulus of Inconel 600 at various temperatures are as follows:
• At 20°C (room temperature), the elastic modulus is approximately 200 GPa.
• At 200°C, it decreases to about 190 GPa
.• At 400°C, it is around 180 GPa.
• At 600°C, the modulus drops to roughly 165 GPa.
• At 800°C, it is approximately 145 GPa.
• At 1000°C, the elastic modulus of Inconel 600 is about 120 GPa.
These values are representative for the annealed condition and may vary slightly depending on factors such as heat treatment, cold work, and manufacturing processes. The decrease in modulus with temperature is primarily due to increased atomic mobility and softening of the material's microstructure.
info-345-347info-352-351
info-352-351info-348-348
2.Does the hardness of Inconel 600 change with heat treatment?
Yes, the hardness of Inconel 600 is significantly influenced by heat treatment. Inconel 600 is a solid-solution strengthened alloy, and while it does not undergo a precipitation-hardening reaction like some other nickel-based alloys (e.g., Inconel 718), its hardness is still affected by microstructural changes during heat treatment.
Key points regarding the effect of heat treatment on the hardness of Inconel 600:
• Annealing: Heating to temperatures between 1010°C and 1150°C followed by rapid cooling (usually water quenching) results in a soft, ductile microstructure with reduced hardness. The typical Rockwell hardness (HRB) after annealing is 65–85 HRB
.• Solution Annealing: This process, which is similar to annealing, further homogenizes the microstructure and reduces hardness to its lowest practical level
.• Cold Work + Stress Relief: Cold working increases hardness significantly, but subsequent stress relief annealing (e.g., at 700–900°C) reduces hardness slightly while improving ductility and dimensional stability.
• Aging: Inconel 600 does not form significant precipitates during aging, so aging treatments do not increase hardness as they do in precipitation-hardened alloys. However, prolonged exposure to high temperatures can cause grain growth, which may slightly reduce hardness.
In summary, the hardness of Inconel 600 is most significantly affected by annealing and cold work. Annealing reduces hardness, while cold working increases it. Aging has minimal impact on hardness due to the absence of strengthening precipitates.