Differences Between C12200 and C11000 copper

Key Differences Between C12200 and C11000

C12200 (phosphorus-deoxidized copper) and C11000 (electrolytic tough pitch copper, ETP) are two widely used high-purity copper grades (both ≥99.90% Cu) with distinct chemical compositions, manufacturing processes, and performance characteristics. Below is a detailed comparison across core dimensions, aligned with international standards (ASTM B152, SAE J461, UNS):
Comparison Dimension C12200 (Phosphorus-Deoxidized Copper) C11000 (Electrolytic Tough Pitch Copper, ETP)
1. Chemical Composition - Copper (Cu): 99.90–99.95 wt%
- Key Alloying Element: Phosphorus (P): 0.015–0.040 wt% (primary deoxidizer)
- Oxygen (O): ≤0.001 wt% (ultra-low, removed by P)
- Impurities: Fe ≤0.005 wt%, Pb ≤0.005 wt%, S ≤0.002 wt%
- Copper (Cu): 99.90–99.95 wt%
- Key Alloying Element: Oxygen (O): 0.02–0.05 wt% (added during casting)
- Phosphorus (P): ≤0.004 wt% (trace impurity, strictly controlled)
- Impurities: Fe ≤0.005 wt%, Pb ≤0.005 wt%, Zn ≤0.005 wt%
2. Manufacturing Process - Produced via phosphorus deoxidation: Phosphorus is added during casting to react with oxygen, forming solid phosphorous oxides (e.g., P₂O₅) that are removed as slag.
- No electrolytic refining step is required for deoxidation (though raw copper may still be electrolytically refined for purity).
- Produced via oxygenation (tough pitch process): Oxygen is intentionally added to molten copper to react with impurities (e.g., carbon, sulfur), forming oxides that float to the surface as slag.
- Refined via electrolysis to achieve ≥99.9% Cu purity, followed by oxygen addition during casting.
3. Core Performance Differences
- Weldability Excellent-ultra-low oxygen content eliminates hydrogen embrittlement (cracking in high-temperature/humid welding environments) and weld porosity. Ideal for gas welding, arc welding, and brazing. Poor-oxygen reacts with hydrogen during welding to form H₂O vapor, causing porosity, cracking, and reduced weld strength. Not recommended for high-integrity welding applications.
- Electrical Conductivity Good: ~85–90% IACS (slightly lower than C11000 due to phosphorus, which acts as a conductivity suppressant). Excellent: ~98–100% IACS (among the highest of all copper grades) – oxygen has minimal impact on conductivity, and impurities are tightly controlled.
- Thermal Conductivity Good: ~360–380 W/(m·K) (20°C) – slightly reduced by phosphorus. Excellent: ~390–401 W/(m·K) (20°C) – one of the most thermally conductive commercial metals.
- Ductility & Formability High ductility (elongation at break: ~45–50% in annealed temper) – suitable for bending, stamping, and drawing, but phosphorus may slightly reduce cold workability compared to C11000. Exceptional ductility (elongation at break: ~50–55% in annealed temper) – extremely easy to form, bend, and stamp without cracking.
- Corrosion Resistance - Excellent resistance to general corrosion, freshwater, and mild chemicals.
- Superior to C11000 in hydrogen-containing environments (e.g., refineries, chemical plants) due to no oxygen-induced embrittlement.
- Excellent resistance to atmospheric corrosion, freshwater, and most chemicals.
- Susceptible to hydrogen embrittlement in high-temperature/humid environments with hydrogen (e.g., welding, heat treatment in moist atmospheres).
- Hardness & Strength Annealed temper: ~40–50 HB; Full-hard temper: ~85–95 HB – phosphorus slightly increases strength/hardness compared to C11000. Annealed temper: ~35–45 HB; Full-hard temper: ~80–90 HB – naturally softer than C11000 in the same temper.
4. Typical Applications - Welded components: Heat exchangers, refrigeration tubing, air conditioning coils, and plumbing pipes (especially for welded joints).
- Industrial equipment: Chemical processing valves, marine hardware, and high-pressure gas lines.
- Electrical applications requiring moderate conductivity and weldability (e.g., busbars for welded assemblies).
- Electrical applications: Power cables, wires, electrical contacts, terminals, and busbars (where maximum conductivity is critical).
- Thermal management: Heat sinks, radiators, and heat transfer plates.
- General-purpose: Plumbing pipes (soldered, not welded), sheet metal, fasteners, and decorative components.
5. Standards Compliance ASTM B152, ASTM B124, SAE J461, ISO 13373-1 ASTM B152, ASTM B133, SAE J461, ISO 13373-1

info-445-447info-446-443

info-446-443info-444-444

Summary of Core Distinctions

The primary difference between C12200 and C11000 lies in deoxidation method and oxygen content, which drive their performance tradeoffs:

C12200 uses phosphorus for deoxidation (ultra-low oxygen, moderate conductivity) – optimized for weldability and resistance to hydrogen embrittlement, ideal for welded components and harsh industrial environments.

C11000 uses oxygen for deoxidation (moderate oxygen, maximum conductivity) – optimized for electrical/thermal performance and formability, ideal for conductive, non-welded applications.

Selection depends on key requirements: prioritize C12200 for welding or hydrogen-rich environments; choose C11000 for maximum conductivity, flexibility, or general-purpose non-welded use.
 