Why ASTM B168 Is the Reference Standard for Inconel 600 Plate and Sheet
ASTM B168 is the specification for nickel-chromium-iron alloy plate, sheet and strip, and it is the document that buyers, mills and third-party inspectors return to when a project needs one auditable definition of what the material is. Inconel 600 appears under this specification as UNS N06600, with the European designation Werkstoff 2.4816 (NiCr15Fe). The alloy is a solid-solution strengthened nickel-chromium-iron material with roughly 76 % nickel, 15.5 % chromium and 8 % iron in the matrix.
Because the alloy depends on chemistry and annealing condition rather than on a precipitation-hardening treatment, plate and sheet properties are stable, predictable and easy to weld. That combination is why the product is specified for furnace internals, heat exchanger tubing and shells, chemical process vessels, nuclear components and electrical resistance hardware.
ASTM B168 covers several closely related grades, including UNS N06600, N06601, N06603, N06690 and N06693. For Inconel 600 the controlling UNS number is N06600, and that is the number an inspector will look for on the mill certificate.
Chemical Composition of UNS N06600 Under ASTM B168
The limits below are the heat-analysis values a melt must meet for the product to be certified as UNS N06600. Product analysis tolerances apply at the edges of each range.
| Element | Requirement, % | What It Does |
|---|---|---|
| Nickel (Ni) | 72.0 min | Austenitic matrix; resistance to chloride stress corrosion cracking |
| Chromium (Cr) | 14.0 to 17.0 | Oxidation and hot corrosion resistance |
| Iron (Fe) | 6.0 to 10.0 | Matrix balance and cost control |
| Carbon (C) | 0.15 max | Strength; capped for weldability |
| Manganese (Mn) | 1.0 max | Deoxidation |
| Silicon (Si) | 0.5 max | Deoxidation |
| Copper (Cu) | 0.5 max | Residual element |
| Sulfur (S) | 0.015 max | Hot workability and cleanliness |
Mechanical Properties of Annealed Plate and Sheet
Plate is normally supplied hot rolled and annealed; sheet is cold rolled and annealed and then pickled or bright annealed. The table below lists the room-temperature levels normally required for annealed UNS N06600 product.
| Property | Typical minimum, annealed | Note |
|---|---|---|
| Tensile strength | 550 MPa (80 ksi) | Room temperature |
| Yield strength, 0.2 % offset | 240 MPa (35 ksi) | Room temperature |
| Elongation | 30 % | Ductility in tension |
| Hardness | Reported as produced | Normally informational rather than a rejection basis |
Two other quality points matter in practice. First, grain size is reported on the certificate because coarse grains improve creep behaviour while fine grains improve fatigue behaviour. Second, the annealed condition is what gives the material its ductility, so a plate that has been straightened or locally heated without a controlled anneal can show distorted properties even though the chemistry is correct.
Thickness, Width and Finish Availability
Cold-rolled sheet is generally produced from about 0.3 mm up to roughly 6 mm, in widths to around 1500 mm and in coil or cut lengths. Hot-rolled plate runs from about 6 mm to 100 mm and heavier on request, supplied as cut lengths, water-jet blanks or plasma-cut profiles. Standard finishes include hot-rolled annealed and pickled, cold-rolled and bright annealed, and cold-rolled, annealed and pickled. No. 1 and 2D finishes suit process equipment, while a 2B or bright finish is usual when appearance or cleanability matters. Widths, edge condition and flatness tolerances should be stated on the order, because plate cut from a wide coil and plate rolled to width can differ in residual stress.
Corrosion and High-Temperature Performance
Inconel 600 resists oxidation in air at continuous service temperatures up to about 1093 C (2000 F). It also tolerates carburizing and nitriding atmospheres, which is why it is used for retorts, muffle furnaces and heat-treat fixtures. In chloride-bearing water the high nickel content makes the alloy essentially immune to chloride stress corrosion cracking under conditions that would crack austenitic stainless steel, and it handles caustic and many organic media well.
Two limits deserve attention. The first is sulfur. In strongly sulfidizing atmospheres at elevated temperature the alloy can suffer accelerated attack, and a higher-chromium grade should be considered. The second is aqueous service in strongly oxidizing acids, where higher-molybdenum or higher-chromium alloys are usually a better fit. Selecting the grade on the actual chemistry of the process stream, rather than on temperature alone, avoids most field failures.
Typical Applications
Common end uses include furnace muffles, retorts, radiant tubes and heating element sheaths; heat exchanger baffles, shells and tube sheets; reactor internals and nuclear steam generator components; caustic evaporator parts; and food processing equipment where freedom from metallic contamination is required. The alloy is also used for bolts and springs in hot gas paths, although bar product rather than plate or sheet is the usual form for those items.
How to Specify an Order
A complete enquiry should state the specification and UNS number, the product form and condition, the dimensions with tolerances, the finish, the heat treatment condition, the test requirements such as tension and grain size, any additional examinations such as ultrasonic or liquid penetrant testing, and the documentation package including the mill certificate to EN 10204 3.1. Where a second standard applies, such as an ASME code case or a project specification, it should be named alongside ASTM B168 so the mill can plan a single melting and rolling route. Sample sizes for destructive testing should also be agreed in advance, since plate is expensive and re-testing disrupts a schedule.
Frequently Asked Questions About ASTM B168 Inconel 600 Plate
Q: What is the difference between Inconel 600 sheet and plate under ASTM B168?
A: The alloy is the same and the chemistry limits are the same; the difference is the product form and the thickness range. Sheet is cold rolled to thinner gauges and supplied in coil or cut lengths, while plate is hot rolled at heavier thicknesses and generally needs a separate annealing and ultrasonic testing route.
Q: What maximum temperature can Inconel 600 plate be used at?
A: In air, oxidation resistance is generally quoted up to about 1093 C (2000 F) for continuous service. The practical limit is usually set by the mechanical load, the atmosphere and the required service life rather than by the alloy itself, and sulfidizing atmospheres need special consideration.
Q: Is Inconel 600 magnetic?
A: The annealed alloy is weakly magnetic and becomes slightly more magnetic after cold working. This is a normal characteristic of the nickel-chromium-iron system and is not a defect or a sign of the wrong grade.
Q: Can Inconel 600 plate be welded without post-weld heat treatment?
A: Yes. The alloy is readily welded by common arc processes, and matching or nickel-based filler metals are used for full-strength joints. Post-weld heat treatment is normally unnecessary for plate and sheet, although a solution anneal may be specified where the joint will see severe high-temperature service.
Q: What is the Werkstoff number for Inconel 600, and does it equal UNS N06600?
A: The European designation is Werkstoff 2.4816, also written NiCr15Fe. It describes the same composition family as UNS N06600, but the two systems are not interchangeable documents, so a buyer should always quote the specification that must appear on the certificate.
Q: How is ASTM B168 Inconel 600 plate priced compared with standard stainless steel?
A: Pricing follows the nickel and chromium content together with the production route, so the alloy sits well above austenitic stainless steel per kilogram. Buyers should compare on a delivered-cost-per-part basis, because the longer service life and lower maintenance demand often offset the higher metal price.