Uns N19907 Superalloy Sheet For Gas Turbine Seals Incoloy Nickel Alloy 907 Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Alloy 907 (Incoloy alloy 907) is a nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of alloy 903 but alloy 907 has improved notch-rupture properties at elevated temperatures. Alloy 907 is used for gas turbines components (seals, shafts, casings and other structural parts).
Incoloy 907 Application
▪ Gas turbine seals
▪ Casings
▪ Glass to metal sealing
Machinability
Incoloy 907 can be machined using conventional machining methods which are used for iron-based alloys. Machining operations are performed using commercial coolants. High-speed operations such as grinding, milling or turning, are performed using water-base coolants.
Specifications:
▪ UNS N19907
▪ Incoloy Alloy 907
Incoloy 907 Chemical Composition
| Elements | Content (%) |
| Iron, Fe | 42 |
| Nickel, Ni | 38 |
| Cobalt, Co | 13 |
| Niobium, Nb | 4.7 |
| Titanium, Ti | 1.5 |
| Silicon, Si | 0.15 |
| Aluminum, Al | 0.03 |
Incoloy 907 Mechanical Properties
| Properties | Metric | Imperial |
| Tensile strength (precipitation hardened, value at room temperature) | 1350 MPa | 196000 psi |
| Yield strength (@ strain 0.200%, precipitation hardened, value at room temperature) | 1100 MPa | 160000 psi |
| Poisson's ratio | 0.36 | 0.36 |
| Elongation at break (precipitation hardened) | 10% | 10% |
| Reduction of area | 36 | 36 |
Available Sizes And Specifications
| Alloy 907 available sizes and specifications | |
| Grade | Alloy 907 |
| Nickel plate | Thickness: 0.3mm - 150.0mm Width: 1000mm - 3000mm |
| Nickel strip/ nickel foil | Thickness: 0.02mm - 16.0mm Width: 5mm - 3000mm |
| Nickel coil | Thickness: 0.3mm - 16.0mm Width: 1000mm - 3000mm |
| Nickel pipe | Outside diameter: 6mm - 1219mm Thickness: 0.5mm - 100mm |
| Nickel Capillary Pipe | Outside diameter: 0.5mm - 6.0mm Thickness: 0.05mm - 2.0mm |
| Nickel bar | Diameter: Ф4mm - Ф600mm |
| Nickel wire rod | Diameter:Ф0.01mm - Ф6mm |
Our Company


Hot Tags: uns n19907 superalloy sheet for gas turbine seals incoloy nickel alloy 907 plate, China uns n19907 superalloy sheet for gas turbine seals incoloy nickel alloy 907 plate suppliers, incoloy alloy ductility, incoloy alloy type, incoloy alloy standard, alloy 825 material, incoloy alloy reliability, incoloy alloy goal
You Might Also Like
Send Inquiry